Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 6061-T6 stronger than SLA Resin Tough 2000?
Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against 40.4 MPa for SLA Resin Tough 2000 (6.83x).
Which is lighter, Aluminum 6061-T6 or SLA Resin Tough 2000?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.
Which is stiffer, Aluminum 6061-T6 or SLA Resin Tough 2000?
Aluminum 6061-T6 is stiffer: Young's modulus 68.3 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Aluminum 6061-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6061-T6 or SLA Resin Tough 2000?
For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 6061-T6
SLA Resin Tough 2000
Stiff rod or tie (tension)
lighter
15.3x heavier
Stiff beam (bending)
lighter
2.49x heavier
Stiff panel or plate
lighter
36% heavier
Strong rod or tie
lighter
2.76x heavier
Strong beam
lighter
45% heavier
Strong panel or plate
lighter
6% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6061-T6 or SLA Resin Tough 2000?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 17% for Aluminum 6061-T6.
Thermal
Which expands less with temperature?
Aluminum 6061-T6 expands less: 23.6 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.