Materials / Compare

Aluminum 6061-T6 vs. Steel A992

Compare Aluminum 6061-T6 vs. Steel A992 strength, stiffness, weight and thermal properties.

Aluminum 6061-T6Wrought
Steel A992Wrought
MechanicalAluminum 6061-T6Steel A992
Yield strength276MPa1385MPa239% stronger
Ultimate tensile strength310MPa1505MPa21.63x stronger
Elongation at break17%124.2%242% more ductile
Young's modulus (stiffness)68.3GPa1design value200GPa3
Density2,700kg/m³12.91x lighter7,850kg/m³4
Strength to weight102kN·m/kg2.08x higher49kN·m/kg
Stiffness to weight25.3MN·m/kg25.5MN·m/kg
Poisson's ratio0.335design value0.33
Shear modulus25.7GPa76.9GPa3x stiffer in shear
Bulk modulus67GPa167GPa2.49x higher
Speed of sound5,030m/s5,048m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Steel A992
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Steel A992
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 6061-T6Steel A992
Thermal conductivity167W/m·K13.48x more heat through a fin48W/m·K4
Thermal expansion23.6µm/m·K112µm/m·K41.97x less
100 mm part over a 50 °C swing118µm growth60µm growth1.97x less
Specific heat896J/kg·K1base material460–480J/kg·K6
Heats up and cools (diffusivity)69mm²/s5.31x faster13mm²/s
Thermal shock resistance19,159W/m3.55x more resistant5,390W/m
Melting pointsolidus-liquidus582–652°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Steel A992
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Steel A992
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: Kaiser Aluminum, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), U.S. Department of Defense, Ovako
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
  1. 1
    Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
  2. 2
    Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
  3. 3
    ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
  4. 4
    Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
  5. 5
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
  6. 6
    S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 6061-T6 stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against 276 MPa for Aluminum 6061-T6 (39%).

Which is lighter, Aluminum 6061-T6 or Steel A992?

Aluminum 6061-T6 is lighter: 2,700 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Aluminum 6061-T6 or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 68.3 GPa for Aluminum 6061-T6, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Aluminum 6061-T6 or Steel A992?

For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 6061-T6Steel A992
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)lighter1.7x heavier
Stiff panel or platelighter2.03x heavier
Strong rod or tielighter2.08x heavier
Strong beamlighter2.33x heavier
Strong panel or platelighter2.46x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 6061-T6 or Steel A992?

Steel A992 stretches further before it breaks: 24.2% elongation at break against 17% for Aluminum 6061-T6.

Thermal

Which conducts heat better, Aluminum 6061-T6 or Steel A992?

Aluminum 6061-T6 conducts heat better: 167 W/m·K against 48 W/m·K for Steel A992.

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 23.6 µm/m·K for Aluminum 6061-T6.

Related comparisons