Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, Röhm, U.S. Department of Defense
Aluminum 7075-T6
7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
1
Alloy 7075 Rod & Bar Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 7075-T6 · Ultimate tensile strength: typicalAluminum 7075-T6 · Elongation at break: typical, in 4DAluminum 7075-T6 · Young's modulus (stiffness): typical
2
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7075-T6 stronger than Plastic PMMA?
Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against tensile strength 80 MPa for Plastic PMMA (6.29x).
Which is lighter, Aluminum 7075-T6 or Plastic PMMA?
Plastic PMMA is lighter: 1,190 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.
Which is stiffer, Aluminum 7075-T6 or Plastic PMMA?
Aluminum 7075-T6 is stiffer: Young's modulus 71 GPa against 3.3 GPa for Plastic PMMA, so the same part in Aluminum 7075-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 7075-T6 or Plastic PMMA?
For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7075-T6
Plastic PMMA
Stiff rod or tie (tension)
lighter
9.14x heavier
Stiff beam (bending)
lighter
1.97x heavier
Stiff panel or plate
lighter
18% heavier
Strong rod or tie
lighter
2.67x heavier
Strong beam
lighter
45% heavier
Strong panel or plate
lighter
7% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7075-T6 or Plastic PMMA?
Aluminum 7075-T6 stretches further before it breaks: 11% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Aluminum 7075-T6 or Plastic PMMA?
Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Aluminum 7075-T6 expands less: 23.4 µm/m·K against 70 µm/m·K for Plastic PMMA.