Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, ATI, U.S. Department of Defense, Steel Construction Institute
Aluminum 7075-T6
7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
Alloy 7075 Rod & Bar Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 7075-T6 · Ultimate tensile strength: typicalAluminum 7075-T6 · Elongation at break: typical, in 4DAluminum 7075-T6 · Young's modulus (stiffness): typical
2
ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
3
Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)
5
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7075-T6 stronger than Stainless Steel 316?
Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 265 MPa for Stainless Steel 316 (1.9x).
Which is lighter, Aluminum 7075-T6 or Stainless Steel 316?
Aluminum 7075-T6 is lighter: 2,800 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, Aluminum 7075-T6 or Stainless Steel 316?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 71 GPa for Aluminum 7075-T6, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, Aluminum 7075-T6 or Stainless Steel 316?
For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7075-T6
Stainless Steel 316
Stiff rod or tie (tension)
lighter
2% heavier
Stiff beam (bending)
lighter
1.71x heavier
Stiff panel or plate
lighter
2.03x heavier
Strong rod or tie
lighter
5.44x heavier
Strong beam
lighter
4.39x heavier
Strong panel or plate
lighter
3.95x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7075-T6 or Stainless Steel 316?
Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 11% for Aluminum 7075-T6.
Thermal
Which conducts heat better, Aluminum 7075-T6 or Stainless Steel 316?
Aluminum 7075-T6 conducts heat better: 130 W/m·K against 14.6 W/m·K for Stainless Steel 316.
Which expands less with temperature?
Stainless Steel 316 expands less: 16.5 µm/m·K against 23.4 µm/m·K for Aluminum 7075-T6.