Materials / Compare

Aluminum A380 vs. Drywall

Compare Aluminum A380 vs. Drywall strength, stiffness, weight and thermal properties.

Aluminum A380Cast
DrywallNatural
MechanicalAluminum A380Drywall
Yield strength160MPa1not given (tensile used)
Ultimate tensile strength320MPa11–2MPa2
Compressive strengthnot sourced2.4MPa3
Elongation at break3.5%1not sourced
Young's modulus (stiffness)71GPa11–2GPa2
Density2,713kg/m³1not sourced
Strength to weight59kN·m/kgnot sourced
Stiffness to weight26.2MN·m/kgnot sourced
Poisson's ratio0.334not sourced
Shear modulus26.7GPanot sourced
Bulk modulus69.6GPanot sourced
Speed of sound5,116m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum A380Drywall
Thermal conductivity96.2W/m·K1not sourced
Thermal expansion21.8µm/m·K116.7µm/m·K330% less
100 mm part over a 50 °C swing109µm growth83.5µm growth30% less
Specific heat963J/kg·K11,090J/kg·K313% higher
Heats up and cools (diffusivity)36.8mm²/snot sourced
Thermal shock resistance6,669W/mnot sourced
Max service temperaturenot sourced52°C5
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Rheocast Company, USDA Forest Products Laboratory, Gypsum Association, North American Die Casting Association, USG
Aluminum A380
A380 aluminium high-pressure die-casting alloy, typical properties; Rheocast Company (aluminium die caster, Germantown WI) A380 alloy data page.
Drywall
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
  1. 1
    Alloy Aluminum: A380Rheocast CompanyAluminum A380 · Yield strength: typical, 25 °CAluminum A380 · Ultimate tensile strength: typical, 25 °CAluminum A380 · Elongation at break: typicalAluminum A380 · Young's modulus (stiffness): typical, 25 °CAluminum A380 · Density: typical at 68 °FAluminum A380 · Thermal conductivity: typical at 68 °FAluminum A380 · Thermal expansion: typical, 68-572 °F (20-300 °C)Aluminum A380 · Specific heat: typical at 68 °F
  2. 2
    Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
  3. 3
    GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
  4. 4
    Product Design for Die Casting, Table 4.1: Die Casting Alloys Material Properties ComparisonNorth American Die Casting Associationarchived copyAluminum A380 · Poisson's ratio: typical, as-cast, separately die cast specimens
  5. 5
    Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum A380 stronger than Drywall?

Aluminum A380 is stronger: its yield strength is 160 MPa against tensile strength 1.5 MPa for Drywall (107x).

Which is stiffer, Aluminum A380 or Drywall?

Aluminum A380 is stiffer: Young's modulus 71 GPa against 1.5 GPa for Drywall, so the same part in Aluminum A380 deflects less under the same load.

Thermal

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 21.8 µm/m·K for Aluminum A380.

Related comparisons