Materials / Compare

Aluminum A380 vs. PCB Board FR-4, 2 copper planes

Compare Aluminum A380 vs. PCB Board FR-4, 2 copper planes strength, stiffness, weight and thermal properties.

Change either side
Aluminum A380Cast
PCB Board FR-4, 2 copper planesComposite
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength160MPasourcetypical, 25 °Cnot given (tensile used)
Ultimate tensile strength320MPasourcetypical, 25 °C246–385MPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D3039)
Elongation at break3.5%sourcetypicalnot sourced
Young's modulus (stiffness)71GPasourcetypical, 25 °C21.9–25.8GPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D790-15e2); the copper planes are left out
Density2,713kg/m³sourcetypical at 68 °Fnot sourced
Strength to weight59kN·m/kgnot sourced
Stiffness to weight26.2MN·m/kgnot sourced
Poisson's rationot sourced0.171–0.177sourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction
Shear modulusnot sourced10.2GPa
Bulk modulusnot sourced12.2GPa
Speed of sound5,116m/snot sourced
Thermal
Thermal conductivity96.2W/m·Ksourcetypical at 68 °Fnot sourced
Thermal expansion21.8µm/m·Ksourcetypical, 68-572 °F (20-300 °C)13–14µm/m·Ksourcethe bare laminate's (fr4-370hr), in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)
100 mm part over a 50 °C swing109µm growth67.5µm growth1.61x less
Specific heat963J/kg·Ksourcetypical at 68 °Fnot sourced
Heats up and cools (diffusivity)36.8mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Values forA380 aluminium high-pressure die-casting alloy, typical properties; Rheocast Company (aluminium die caster, Germantown WI) A380 alloy data page.A whole circuit board read as one orthotropic plate: the JEDEC high-K thermal test board (JESD51-7, "2s2p"), 0.062 in (1.575 mm) thick with two internal solid copper planes 0.0014 in (1 oz) thick, as Texas Instruments SZZA017A Table 1 gives it. Copper C110 and the Isola 370HR laminate from this library; the layers conduct in parallel along the board and in series through it (boardStackup.ts). Its two 0.0028 in trace layers cover little of the board and are left out; vias are ignored. Mechanical values are the bare laminate's.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum A380 stronger than PCB Board FR-4, 2 copper planes?

PCB Board FR-4, 2 copper planes is stronger: its tensile strength is 315 MPa against yield strength 160 MPa for Aluminum A380 (1.97x).

Which is stiffer, Aluminum A380 or PCB Board FR-4, 2 copper planes?

Aluminum A380 is stiffer: Young's modulus 71 GPa against 23.9 GPa for PCB Board FR-4, 2 copper planes, so the same part in Aluminum A380 deflects less under the same load.

Which expands less with temperature?

PCB Board FR-4, 2 copper planes expands less: 13.5 µm/m·K against 21.8 µm/m·K for Aluminum A380.

Among 73 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Strength against density

Related comparisons