Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, LyondellBasell, U.S. Department of Defense, INEOS Olefins & Polymers USA
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
2
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
4
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum stronger than Plastic HDPE?
Aluminum is stronger: its yield strength is 276 MPa against 24 MPa for Plastic HDPE (11.5x).
Which is lighter, Aluminum or Plastic HDPE?
Plastic HDPE is lighter: 950 kg/m³ against 2,700 kg/m³ for Aluminum.
Which is stiffer, Aluminum or Plastic HDPE?
Aluminum is stiffer: Young's modulus 68.3 GPa against 0.9 GPa for Plastic HDPE, so the same part in Aluminum deflects less under the same load.
Which is lighter for the same job, Aluminum or Plastic HDPE?
For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum
Plastic HDPE
Stiff rod or tie (tension)
lighter
26.7x heavier
Stiff beam (bending)
lighter
3.07x heavier
Stiff panel or plate
lighter
49% heavier
Strong rod or tie
lighter
4.05x heavier
Strong beam
lighter
1.79x heavier
Strong panel or plate
lighter
19% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Aluminum or Plastic HDPE?
Aluminum conducts heat better: 167 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Aluminum expands less: 23.6 µm/m·K against 120 µm/m·K for Plastic HDPE.