Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Kaiser Aluminum, Röhm, U.S. Department of Defense
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
2
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum stronger than Plastic PMMA?
Aluminum is stronger: its yield strength is 276 MPa against tensile strength 80 MPa for Plastic PMMA (3.45x).
Which is lighter, Aluminum or Plastic PMMA?
Plastic PMMA is lighter: 1,190 kg/m³ against 2,700 kg/m³ for Aluminum.
Which is stiffer, Aluminum or Plastic PMMA?
Aluminum is stiffer: Young's modulus 68.3 GPa against 3.3 GPa for Plastic PMMA, so the same part in Aluminum deflects less under the same load.
Which is lighter for the same job, Aluminum or Plastic PMMA?
For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic PMMA is lighter for a strong panel or plate.
Part that must be
Aluminum
Plastic PMMA
Stiff rod or tie (tension)
lighter
9.12x heavier
Stiff beam (bending)
lighter
2.01x heavier
Stiff panel or plate
lighter
21% heavier
Strong rod or tie
lighter
1.52x heavier
Strong beam
about equal
about equal
Strong panel or plate
22% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum or Plastic PMMA?
Aluminum stretches further before it breaks: 17% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Aluminum or Plastic PMMA?
Aluminum conducts heat better: 167 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Aluminum expands less: 23.6 µm/m·K against 70 µm/m·K for Plastic PMMA.