Materials / Compare

Aluminum vs. Rubber

Compare Aluminum vs. Rubber strength, stiffness, weight and thermal properties.

AluminumWrought
RubberBulk polymer (molded or machined)
MechanicalAluminumRubber
Yield strength276MPa1not given (tensile used)
Ultimate tensile strength310MPa113.5x stronger23MPa2
Elongation at break17%1830%248.8x more ductile
Young's modulus (stiffness)68.3GPa1not sourced
Density2,700kg/m³1960kg/m³22.81x lighter
Strength to weight102kN·m/kg4.27x higher24kN·m/kg
Stiffness to weight25.3MN·m/kgnot sourced
Poisson's ratio0.333government0.54
Shear modulus25.7GPanot sourced
Bulk modulus67GPanot sourced
Speed of sound5,030m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumRubber
Strength against densityHigher and further left: stronger for its weight
ThermalAluminumRubber
Thermal conductivity167W/m·K11,106x more heat through a fin0.151W/m·K5
Thermal expansion23.6µm/m·K1not sourced
100 mm part over a 50 °C swing118µm growthnot sourced
Specific heat896J/kg·K1government1,881J/kg·K42.1x higher
Heats up and cools (diffusivity)69mm²/s826x faster0.0836mm²/s
Thermal shock resistance19,159W/mnot sourced
Melting pointsolidus-liquidus582–652°C1not sourced
Max service temperaturenot sourced70°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumRubber
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Kaiser Aluminum, Weir Minerals, U.S. Department of Defense, National Institute of Standards and Technology, Defense Technical Information Center
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
Rubber
Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305
  1. 1
    Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
  2. 2
    Linatex Premium Rubber Spec Sheet (WMD0118, 2023)Weir MineralsRubber · Ultimate tensile strength: typicalRubber · Elongation at break: typicalRubber · Density: typical (specific gravity)Rubber · Max service temperature: continuous use operating range
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
  4. 4
    Compressibility of Natural Rubber at Pressures Below 500 kg/cm², J. Res. NBS 68A (1964)National Institute of Standards and Technologyarchived copyRubber · Poisson's ratio: government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation (0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).)Rubber · Specific heat: government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
  5. 5
    Thermal Conductivity of Soft Vulcanized Natural Rubber: Selected Values (AD 643325)Defense Technical Information Centerarchived copyRubber · Thermal conductivity: government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum stronger than Rubber?

Aluminum is stronger: its yield strength is 276 MPa against tensile strength 23 MPa for Rubber (12x).

Which is lighter, Aluminum or Rubber?

Rubber is lighter: 960 kg/m³ against 2,700 kg/m³ for Aluminum.

Which is lighter for the same job, Aluminum or Rubber?

For the same stiffness or strength: Aluminum is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminumRubber
Strong rod or tielighter4.27x heavier
Strong beamlighter1.86x heavier
Strong panel or platelighter23% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 17% for Aluminum.

Thermal

Which conducts heat better, Aluminum or Rubber?

Aluminum conducts heat better: 167 W/m·K against 0.151 W/m·K for Rubber.

Related comparisons