Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
2
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
5
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum stronger than SLA Resin Standard?
Aluminum is stronger: its yield strength is 276 MPa against tensile strength 60 MPa for SLA Resin Standard (4.6x).
Which is lighter, Aluminum or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 2,700 kg/m³ for Aluminum.
Which is stiffer, Aluminum or SLA Resin Standard?
Aluminum is stiffer: Young's modulus 68.3 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Aluminum deflects less under the same load.
Which is lighter for the same job, Aluminum or SLA Resin Standard?
For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; SLA Resin Standard is lighter for a strong panel or plate.
Part that must be
Aluminum
SLA Resin Standard
Stiff rod or tie (tension)
lighter
11.1x heavier
Stiff beam (bending)
lighter
2.23x heavier
Stiff panel or plate
lighter
31% heavier
Strong rod or tie
lighter
2.06x heavier
Strong beam
lighter
24% heavier
Strong panel or plate
4% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum or SLA Resin Standard?
Aluminum stretches further before it breaks: 17% elongation at break against 8% for SLA Resin Standard.
Thermal
Which conducts heat better, Aluminum or SLA Resin Standard?
Aluminum conducts heat better: 167 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Aluminum expands less: 23.6 µm/m·K against 114 µm/m·K for SLA Resin Standard.