Materials / Compare
Brass C260 vs. DMLS 17-4PH Stainless Steel
Compare Brass C260 vs. DMLS 17-4PH Stainless Steel strength, stiffness, weight and thermal properties.
| Mechanical | Brass C260 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Yield strength | 345MPa1 | mean861MPa22.49x stronger |
| Ultimate tensile strength | 427MPa1 | mean886MPa22.07x stronger |
| Elongation at break | 23%116% more ductile | mean at break19.9%2 |
| Young's modulus (stiffness) | 110GPa3 | base material197GPa41.79x stiffer |
| Density | 8,525kg/m³3 | mean part density7,790kg/m³2 |
| Strength to weight | 40.5kN·m/kg | 110kN·m/kg2.73x higher |
| Stiffness to weight | 12.9MN·m/kg | 25.3MN·m/kg1.95x higher |
| Poisson's ratio | 0.345 | base material0.2724 |
| Shear modulus | 41.2GPa | 77.4GPa1.88x stiffer in shear |
| Bulk modulus | 115GPa | 144GPa25% higher |
| Speed of sound | 3,597m/s | 5,029m/s40% faster |
| Thermal | Brass C260 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Thermal conductivity | 121W/m·K36.77x more heat through a fin | base material17.9W/m·K4 |
| Thermal expansion | 20µm/m·K3 | mean 25-100 °C10.4µm/m·K21.92x less |
| 100 mm part over a 50 °C swing | 100µm growth | 52µm growth1.92x less |
| Specific heat | 377J/kg·K3 | base material460J/kg·K422% higher |
| Heats up and cools (diffusivity) | 37.7mm²/s7.55x faster | 5mm²/s |
| Thermal shock resistance | 12,510W/m2.29x more resistant | 5,474W/m |
| Melting point | solidus-liquidus916–954°C3 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Copper Development Association, EOS GmbH, Cleveland-Cliffs, Wieland
- Brass C260
- C26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)
- DMLS 17-4PH Stainless Steel
- EOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8M
- 1Electronic Connector Design Guide: Cold Rolled TempersCopper Development Associationarchived copyBrass C260 · Yield strength: nominal, strip/flat, 0.5% extension (not 0.2% offset)Brass C260 · Ultimate tensile strength: nominal, strip/flatBrass C260 · Elongation at break: nominal, in 2.0 in., strip/flat
- 2EOS StainlessSteel 17-4PH IndustryLine Material Data Sheet, M 290EOS GmbHarchived copyDMLS 17-4PH Stainless Steel · Yield strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Ultimate tensile strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Elongation at break: mean at break, as built, horizontalDMLS 17-4PH Stainless Steel · Density: mean part density (ISO 3369)DMLS 17-4PH Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)
- 3C26000 Alloy (copper.org)Copper Development Associationarchived copyBrass C260 · Young's modulus (stiffness): typical, temper-independentBrass C260 · Density: nominalBrass C260 · Thermal conductivity: typical, 20 °CBrass C260 · Thermal expansion: typical, mean 20-300 °CBrass C260 · Specific heat: typical, 20 °CBrass C260 · Melting point: solidus-liquidus
- 417-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 17-4PH Stainless Steel · Young's modulus (stiffness): base material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Poisson's ratio: base material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Thermal conductivity: base material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Specific heat: base material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)
- 5Wieland-M30 (CuZn30, C26000) Data SheetWielandarchived copyBrass C260 · Poisson's ratio: reference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Brass C260 stronger than DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against 345 MPa for Brass C260 (2.49x).
Which is lighter, Brass C260 or DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel is lighter: 7,790 kg/m³ against 8,525 kg/m³ for Brass C260.
Which is stiffer, Brass C260 or DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel is stiffer: Young's modulus 197 GPa against 110 GPa for Brass C260, so the same part in DMLS 17-4PH Stainless Steel deflects less under the same load.
Which is lighter for the same job, Brass C260 or DMLS 17-4PH Stainless Steel?
For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Brass C260 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Stiff rod or tie (tension) | 1.95x heavier | lighter |
| Stiff beam (bending) | 46% heavier | lighter |
| Stiff panel or plate | 33% heavier | lighter |
| Strong rod or tie | 2.73x heavier | lighter |
| Strong beam | 2.01x heavier | lighter |
| Strong panel or plate | 1.73x heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Brass C260 or DMLS 17-4PH Stainless Steel?
Brass C260 stretches further before it breaks: 23% elongation at break against 19.9% for DMLS 17-4PH Stainless Steel.
Thermal
Which conducts heat better, Brass C260 or DMLS 17-4PH Stainless Steel?
Brass C260 conducts heat better: 121 W/m·K against 17.9 W/m·K for DMLS 17-4PH Stainless Steel.
Which expands less with temperature?
DMLS 17-4PH Stainless Steel expands less: 10.4 µm/m·K against 20 µm/m·K for Brass C260.
Related comparisons
- Brass C260 vs. Brass C360
- Brass C260 vs. Zinc Zamak 3
- Brass C260 vs. Steel AISI 1018
- Brass C260 vs. Steel
- DMLS 17-4PH Stainless Steel vs. Steel AISI 4340
- DMLS 17-4PH Stainless Steel vs. Nickel Inconel 718
- DMLS 17-4PH Stainless Steel vs. Stainless Steel 17-4PH
- DMLS 17-4PH Stainless Steel vs. Steel AISI 1045