Mechanical
Yield strength345MPasourcenominal, strip/flat, 0.5% extension (not 0.2% offset)265MPasourcetypical (representative), annealed 1.0 mm sheet
Ultimate tensile strength427MPasourcenominal, strip/flat583MPasourcetypical (representative), annealed 1.0 mm sheet
Elongation at break23%sourcenominal, in 2.0 in., strip/flat61%sourcetypical (representative), annealed, in 2 in. (51 mm)
Young's modulus (stiffness)110GPasourcetypical, temper-independent200GPasourcetypical, in tension
Density8,525kg/m³sourcenominal8,027kg/m³sourcetypical
Strength to weight40.5kN·m/kg23% higher33kN·m/kg
Stiffness to weight12.9MN·m/kg24.9MN·m/kg1.93x higher
Poisson's ratio0.34sourcereference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)0.3sourcedesign value (structural stainless steels)
Shear modulus41.2GPa76.9GPa1.87x stiffer in shear
Bulk modulus115GPa167GPa
Speed of sound3,597m/s4,992m/s
Thermal
Thermal conductivity121W/m·Ksourcetypical, 20 °C14.6W/m·Ksource20–100 °C
Thermal expansion20µm/m·Ksourcetypical, mean 20-300 °C16.5µm/m·Ksourcemean, 20–100 °C
100 mm part over a 50 °C swing100µm growth82.5µm growth21% less
Specific heat377J/kg·Ksourcetypical, 20 °C450J/kg·Ksourceat 20 °C
Heats up and cools (diffusivity)37.7mm²/s9.33x faster4.04mm²/s
Thermal shock resistance12,510W/m15.2x more resistant821W/m
Melting point916–954°Csourcesolidus-liquidus1,390–1,440°Csourcemelting range
Max service temperaturenot sourced871–899°Csourceoxidation (scaling) limit in air
Values forC26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Brass C260 stronger than Stainless Steel 316?

Brass C260 is stronger: its yield strength is 345 MPa against 265 MPa for Stainless Steel 316 (30%).

Which is lighter, Brass C260 or Stainless Steel 316?

Stainless Steel 316 is lighter: 8,027 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is stiffer, Brass C260 or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 110 GPa for Brass C260, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Brass C260 or Stainless Steel 316?

For the same stiffness or strength: Brass C260 is lighter for a strong rod or tie, strong beam, strong panel or plate; Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beBrass C260Stainless Steel 316
Stiff rod or tie (tension)1.93x heavierlighter
Stiff beam (bending)43% heavierlighter
Stiff panel or plate30% heavierlighter
Strong rod or tielighter23% heavier
Strong beamlighter12% heavier
Strong panel or platelighter7% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Brass C260 or Stainless Steel 316?

Brass C260 conducts heat better: 121 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 20 µm/m·K for Brass C260.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrass C260Stainless Steel 316
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickBrass C260Stainless Steel 316
Strength against density

Related comparisons