Materials / Compare

Brass C360 vs. SLA Resin Tough 2000

Compare Brass C360 vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Brass C360Wrought
SLA Resin Tough 20003D printed (SLA resin)
MechanicalBrass C360SLA Resin Tough 2000
Yield strength310MPa17.67x stronger40.4MPa2
Ultimate tensile strength400MPa19.9x stronger40.4MPa2
Flexural strengthnot sourced67MPa2
Elongation at break25%179%23.16x more ductile
Young's modulus (stiffness)96.5GPa153.6x stiffer1.8GPa2
Density8,498kg/m³11,090kg/m³27.8x lighter
Strength to weight36.5kN·m/kg37.1kN·m/kg2% higher
Stiffness to weight11.4MN·m/kg6.88x higher1.65MN·m/kg
Poisson's ratiobase material0.343not sourced
Shear modulus36GPanot sourced
Bulk modulus101GPanot sourced
Speed of sound3,370m/s2.62x faster1,285m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360SLA Resin Tough 2000
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360SLA Resin Tough 2000
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C360SLA Resin Tough 2000
Thermal conductivity116W/m·K1not sourced
Thermal expansion20.5µm/m·K16.55x lessmean 0-150 °C134µm/m·K2
100 mm part over a 50 °C swing103µm growth6.55x less671µm growth
Specific heat377J/kg·K1not sourced
Heats up and cools (diffusivity)36.2mm²/snot sourced
Thermal shock resistance11,997W/mnot sourced
Melting pointsolidus-liquidus888–899°C1not sourced
Glass transitionnot sourcedDMA112°C2
Max service temperaturenot sourcedHDT 1.8 MPa57°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Copper Development Association, Formlabs, Wieland
Brass C360
C36000 free-cutting brass, H02 half-hard rod 1 in. section (20% cold work), copper.org typical values
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
  1. 1
    C36000 Alloy (copper.org)Copper Development Associationarchived copyBrass C360 · Yield strength: typical, 0.5% extension under loadBrass C360 · Ultimate tensile strength: typicalBrass C360 · Elongation at break: typical, 1 in. rodBrass C360 · Young's modulus (stiffness): typical, temper-independentBrass C360 · Density: nominalBrass C360 · Thermal conductivity: typical, 20 °CBrass C360 · Thermal expansion: typical, mean 20-300 °CBrass C360 · Specific heat: typical, 20 °CBrass C360 · Melting point: solidus-liquidus
  2. 2
    Tough 2000 Resin V2 Technical Data Sheet (2025)Formlabsarchived copySLA Resin Tough 2000 · Yield strength: typicalSLA Resin Tough 2000 · Ultimate tensile strength: typicalSLA Resin Tough 2000 · Flexural strength: typicalSLA Resin Tough 2000 · Elongation at break: typicalSLA Resin Tough 2000 · Young's modulus (stiffness): typicalSLA Resin Tough 2000 · Density: typicalSLA Resin Tough 2000 · Thermal expansion: mean 0-150 °CSLA Resin Tough 2000 · Glass transition: DMASLA Resin Tough 2000 · Max service temperature: HDT 1.8 MPa
  3. 3
    Wieland-Z30 (CuZn39Pb2, C37700) Data SheetWielandarchived copyBrass C360 · Poisson's ratio: base material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Brass C360 stronger than SLA Resin Tough 2000?

Brass C360 is stronger: its yield strength is 310 MPa against 40.4 MPa for SLA Resin Tough 2000 (7.67x).

Which is lighter, Brass C360 or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 8,498 kg/m³ for Brass C360.

Which is stiffer, Brass C360 or SLA Resin Tough 2000?

Brass C360 is stiffer: Young's modulus 96.5 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Brass C360 deflects less under the same load.

Which is lighter for the same job, Brass C360 or SLA Resin Tough 2000?

For the same stiffness or strength: Brass C360 is lighter for a stiff rod or tie (tension); SLA Resin Tough 2000 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beBrass C360SLA Resin Tough 2000
Stiff rod or tie (tension)lighter6.88x heavier
Stiff beam (bending)6% heavierlighter
Stiff panel or plate2.07x heavierlighter
Strong rod or tie2% heavierlighter
Strong beam2x heavierlighter
Strong panel or plate2.81x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Brass C360 or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 25% for Brass C360.

Thermal

Which expands less with temperature?

Brass C360 expands less: 20.5 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.