Materials / Compare

Brick vs. Plastic Nylon PA66

Compare Brick vs. Plastic Nylon PA66 strength, stiffness, weight and thermal properties.

BrickNatural
Plastic Nylon PA66Bulk polymer (molded or machined)
MechanicalBrickPlastic Nylon PA66
Yield strengthnone (brittle)85MPa1
Ultimate tensile strengthmodulus of rupture5.1MPa2not stated (yield given)
Compressive strength77.9MPa3not sourced
Elongation at breaknone (brittle)30%1
Young's modulus (stiffness)not sourced3GPa1
Density2,082kg/m³41,130kg/m³11.84x lighter
Strength to weight2.45kN·m/kg75.2kN·m/kg30.7x higher
Stiffness to weightnot sourced2.65MN·m/kg
Poisson's rationot sourcedbase material0.45
Shear modulusnot sourced1.07GPa
Bulk modulusnot sourced5GPa
Speed of soundnot sourced1,629m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA66
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon PA66
Strength against densityHigher and further left: stronger for its weight
ThermalBrickPlastic Nylon PA66
Thermal conductivity0.92–1.12W/m·K40.33W/m·K1
Thermal expansion7.2µm/m·K313.6x lesslongitudinal98µm/m·K1
100 mm part over a 50 °C swing36µm growth13.6x less490µm growth
Specific heat837J/kg·K61,700J/kg·K12.03x higher
Heats up and cools (diffusivity)0.585mm²/s3.41x faster0.172mm²/s
Thermal shock resistancenot sourced57.2W/m
Melting pointnot sourcedDSC260°C1
Max service temperaturenot sourced101°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon PA66
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickPlastic Nylon PA66
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: BASF, National Institute of Standards and Technology, Brick Industry Association, Covestro
Brick
Solid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonry
Plastic Nylon PA66
BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
  1. 1
    Ultramid A3K Product InformationBASFPlastic Nylon PA66 · Yield strength: typical, dryPlastic Nylon PA66 · Elongation at break: nominal strain at break, dryPlastic Nylon PA66 · Young's modulus (stiffness): typical, dryPlastic Nylon PA66 · Density: typicalPlastic Nylon PA66 · Thermal conductivity: typicalPlastic Nylon PA66 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA66 · Specific heat: typicalPlastic Nylon PA66 · Melting point: DSCPlastic Nylon PA66 · Max service temperature: IEC 60216 temperature index, 20000 h
  2. 2
    Strength of Masonry Walls Under Compressive and Transverse Loads (Building Science Series 34)National Institute of Standards and Technologyarchived copyBrick · Ultimate tensile strength: modulus of rupture (no direct tensile value)
  3. 3
    Technical Notes 3A: Brick Masonry Material PropertiesBrick Industry AssociationBrick · Compressive strength: mean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)Brick · Thermal expansion: TMS Code average coefficient, clay/shale unit masonry
  4. 4
    Technical Notes 4: Introduction to Energy Performance of Brick Masonry (2016)Brick Industry Associationarchived copyBrick · Density: face brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)Brick · Thermal conductivity: range for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)
  5. 5
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  6. 6
    Technical Notes 4B: Energy Code Compliance of Brick Masonry WallsBrick Industry Associationarchived copyBrick · Specific heat: value used in BIA heat-capacity sample calculation

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Brick stronger than Plastic Nylon PA66?

Plastic Nylon PA66 is stronger: its yield strength is 85 MPa against tensile strength 5.1 MPa for Brick (16.7x).

Which is lighter, Brick or Plastic Nylon PA66?

Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 2,082 kg/m³ for Brick.

Which is lighter for the same job, Brick or Plastic Nylon PA66?

For the same stiffness or strength: Plastic Nylon PA66 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beBrickPlastic Nylon PA66
Strong rod or tie30.7x heavierlighter
Strong beam12x heavierlighter
Strong panel or plate7.52x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Brick or Plastic Nylon PA66?

Brick conducts heat better: 1.02 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.

Which expands less with temperature?

Brick expands less: 7.2 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.

Related comparisons