Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources9 documents: LyondellBasell, National Ready Mixed Concrete Association, Federal Highway Administration, Oak Ridge National Laboratory, INEOS Olefins & Polymers USA, USDA Forest Products Laboratory, National Institute of Standards and Technology
Concrete
Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
1
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
CIP 35: Testing Compressive Strength of ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Compressive strength: specified compressive strength class (f'c), not a measured typical
CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
5
The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
6
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
9
Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Which is lighter, Concrete or Plastic HDPE?
Plastic HDPE is lighter: 950 kg/m³ against 2,320 kg/m³ for Concrete.
Which is stiffer, Concrete or Plastic HDPE?
Concrete is stiffer: Young's modulus 25.1 GPa against 0.9 GPa for Plastic HDPE, so the same part in Concrete deflects less under the same load.
Which is lighter for the same job, Concrete or Plastic HDPE?
For the same stiffness or strength: Concrete is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be
Concrete
Plastic HDPE
Stiff rod or tie (tension)
lighter
11.4x heavier
Stiff beam (bending)
lighter
2.16x heavier
Stiff panel or plate
lighter
24% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Concrete or Plastic HDPE?
Concrete conducts heat better: 0.9 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Concrete expands less: 10 µm/m·K against 120 µm/m·K for Plastic HDPE.