Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Copper Development Association, Sumitomo Chemical, Wieland
Copper C10100
C10100 oxygen-free electronic (OFE) copper, annealed to 0.050 mm grain size (OS050), 0.04 in. flat products, copper.org typical values
Plastic LCP GF30
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
1
C10100 Alloy (copper.org)Copper Development Associationarchived copyCopper C10100 · Yield strength: typical, 0.5% extension under load, 0.04 in. flatCopper C10100 · Ultimate tensile strength: typical, 0.04 in. flatCopper C10100 · Elongation at break: typical, 0.04 in. flatCopper C10100 · Young's modulus (stiffness): typicalCopper C10100 · Density: nominalCopper C10100 · Thermal conductivity: typical, 20 °CCopper C10100 · Thermal expansion: typical, mean 20-100 °CCopper C10100 · Specific heat: typical, 20 °CCopper C10100 · Melting point: melting point (liquidus = solidus, pure copper)
2
SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
3
Wieland-K09 (Cu-OFE, C10100) Data SheetWielandCopper C10100 · Poisson's ratio: reference value at room temperature (Wieland-K09 = Cu-OFE = C10100, rolled products)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Copper C10100 stronger than Plastic LCP GF30?
Plastic LCP GF30 is stronger: its tensile strength is 115 MPa against yield strength 69 MPa for Copper C10100 (1.67x).
Which is lighter, Copper C10100 or Plastic LCP GF30?
Plastic LCP GF30 is lighter: 1,610 kg/m³ against 8,941 kg/m³ for Copper C10100.
Which is stiffer, Copper C10100 or Plastic LCP GF30?
Copper C10100 is stiffer: Young's modulus 117 GPa against 11.5 GPa for Plastic LCP GF30, so the same part in Copper C10100 deflects less under the same load.
Which is lighter for the same job, Copper C10100 or Plastic LCP GF30?
For the same stiffness or strength: Copper C10100 is lighter for a stiff rod or tie (tension); Plastic LCP GF30 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Copper C10100
Plastic LCP GF30
Stiff rod or tie (tension)
lighter
1.84x heavier
Stiff beam (bending)
1.74x heavier
lighter
Stiff panel or plate
2.56x heavier
lighter
Strong rod or tie
9.26x heavier
lighter
Strong beam
7.81x heavier
lighter
Strong panel or plate
7.17x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Copper C10100 or Plastic LCP GF30?
Copper C10100 stretches further before it breaks: 45% elongation at break against 1.5% for Plastic LCP GF30.
Thermal
Which conducts heat better, Copper C10100 or Plastic LCP GF30?
Copper C10100 conducts heat better: 391 W/m·K against 0.5 W/m·K for Plastic LCP GF30.
Which expands less with temperature?
Copper C10100 expands less: 16.9 µm/m·K against 20 µm/m·K for Plastic LCP GF30.