Materials / Compare

Copper C110 vs. DMLS 17-4PH Stainless Steel

Compare Copper C110 vs. DMLS 17-4PH Stainless Steel strength, stiffness, weight and thermal properties.

Copper C110Wrought
DMLS 17-4PH Stainless Steel3D printed metal (DMLS)
MechanicalCopper C110DMLS 17-4PH Stainless Steel
Yield strength69MPa1mean861MPa212.5x stronger
Ultimate tensile strength221MPa1mean886MPa24.01x stronger
Elongation at break55%12.76x more ductilemean at break19.9%2
Young's modulus (stiffness)117GPa1base material197GPa31.68x stiffer
Density8,913kg/m³1mean part density7,790kg/m³214% lighter
Strength to weight7.74kN·m/kg110kN·m/kg14.3x higher
Stiffness to weight13.1MN·m/kg25.3MN·m/kg1.92x higher
Poisson's ratio0.344base material0.2723
Shear modulus43.7GPa77.4GPa1.77x stiffer in shear
Bulk modulus122GPa144GPa18% higher
Speed of sound3,626m/s5,029m/s39% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110DMLS 17-4PH Stainless Steel
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110DMLS 17-4PH Stainless Steel
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C110DMLS 17-4PH Stainless Steel
Thermal conductivity391W/m·K121.8x more heat through a finbase material17.9W/m·K3
Thermal expansion16.9µm/m·K1mean 25-100 °C10.4µm/m·K21.62x less
100 mm part over a 50 °C swing84.5µm growth52µm growth1.63x less
Specific heat385J/kg·K1base material460J/kg·K319% higher
Heats up and cools (diffusivity)114mm²/s22.8x faster5mm²/s
Thermal shock resistance8,992W/m1.64x more resistant5,474W/m
Melting pointsolidus-liquidus1,065–1,083°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110DMLS 17-4PH Stainless Steel
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110DMLS 17-4PH Stainless Steel
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Copper Development Association, EOS GmbH, Cleveland-Cliffs, Wieland
Copper C110
C11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical values
DMLS 17-4PH Stainless Steel
EOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8M
  1. 1
    C11000 Alloy (copper.org)Copper Development Associationarchived copyCopper C110 · Yield strength: typical, 0.5% extension under loadCopper C110 · Ultimate tensile strength: typicalCopper C110 · Elongation at break: typical, 1 in. rodCopper C110 · Young's modulus (stiffness): typicalCopper C110 · Density: nominalCopper C110 · Thermal conductivity: typical, 20 °CCopper C110 · Thermal expansion: typical, mean 20-100 °CCopper C110 · Specific heat: typical, 20 °CCopper C110 · Melting point: solidus-liquidus
  2. 2
    EOS StainlessSteel 17-4PH IndustryLine Material Data Sheet, M 290EOS GmbHarchived copyDMLS 17-4PH Stainless Steel · Yield strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Ultimate tensile strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Elongation at break: mean at break, as built, horizontalDMLS 17-4PH Stainless Steel · Density: mean part density (ISO 3369)DMLS 17-4PH Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)
  3. 3
    17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 17-4PH Stainless Steel · Young's modulus (stiffness): base material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Poisson's ratio: base material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Thermal conductivity: base material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Specific heat: base material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)
  4. 4
    Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Copper C110 stronger than DMLS 17-4PH Stainless Steel?

DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against 69 MPa for Copper C110 (12.5x).

Which is lighter, Copper C110 or DMLS 17-4PH Stainless Steel?

DMLS 17-4PH Stainless Steel is lighter: 7,790 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or DMLS 17-4PH Stainless Steel?

DMLS 17-4PH Stainless Steel is stiffer: Young's modulus 197 GPa against 117 GPa for Copper C110, so the same part in DMLS 17-4PH Stainless Steel deflects less under the same load.

Which is lighter for the same job, Copper C110 or DMLS 17-4PH Stainless Steel?

For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110DMLS 17-4PH Stainless Steel
Stiff rod or tie (tension)1.92x heavierlighter
Stiff beam (bending)48% heavierlighter
Stiff panel or plate36% heavierlighter
Strong rod or tie14.3x heavierlighter
Strong beam6.15x heavierlighter
Strong panel or plate4.04x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C110 or DMLS 17-4PH Stainless Steel?

Copper C110 stretches further before it breaks: 55% elongation at break against 19.9% for DMLS 17-4PH Stainless Steel.

Thermal

Which conducts heat better, Copper C110 or DMLS 17-4PH Stainless Steel?

Copper C110 conducts heat better: 391 W/m·K against 17.9 W/m·K for DMLS 17-4PH Stainless Steel.

Which expands less with temperature?

DMLS 17-4PH Stainless Steel expands less: 10.4 µm/m·K against 16.9 µm/m·K for Copper C110.