Materials / Compare

Copper C110 vs. Plastic POM/Acetal

Compare Copper C110 vs. Plastic POM/Acetal strength, stiffness, weight and thermal properties.

Copper C110Wrought
Plastic POM/AcetalBulk polymer (molded or machined)
MechanicalCopper C110Plastic POM/Acetal
Yield strength69MPa169MPa2
Ultimate tensile strength221MPa13.2x stronger69MPa2
Compressive strengthnot sourced124MPa2
Flexural strengthnot sourced99MPa2
Elongation at break55%175%236% more ductile
Young's modulus (stiffness)117GPa141.9x stiffer2.8GPa2
Density8,913kg/m³11,420kg/m³36.28x lighter
Strength to weight7.74kN·m/kg48.6kN·m/kg6.28x higher
Stiffness to weight13.1MN·m/kg6.67x higher1.97MN·m/kg
Poisson's ratio0.3440.352
Shear modulus43.7GPa42.2x stiffer in shear1.04GPa
Bulk modulus122GPa39.2x higher3.11GPa
Speed of sound3,626m/s2.58x faster1,404m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic POM/Acetal
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic POM/Acetal
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C110Plastic POM/Acetal
Thermal conductivity391W/m·K1978x more heat through a fin0.4W/m·K2
Thermal expansion16.9µm/m·K17.22x lessmean122µm/m·K2
100 mm part over a 50 °C swing84.5µm growth7.22x less610µm growth
Specific heat385J/kg·K1average -18 to 100 °C1,465J/kg·K23.8x higher
Heats up and cools (diffusivity)114mm²/s592x faster0.192mm²/s
Thermal shock resistance8,992W/m171x more resistant52.5W/m
Melting pointsolidus-liquidus1,065–1,083°C1175°C2
Max service temperaturenot sourcedHDT 1.8 MPa125°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic POM/Acetal
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic POM/Acetal
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Copper Development Association, DuPont, Wieland
Copper C110
C11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical values
Plastic POM/Acetal
DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com
  1. 1
    C11000 Alloy (copper.org)Copper Development Associationarchived copyCopper C110 · Yield strength: typical, 0.5% extension under loadCopper C110 · Ultimate tensile strength: typicalCopper C110 · Elongation at break: typical, 1 in. rodCopper C110 · Young's modulus (stiffness): typicalCopper C110 · Density: nominalCopper C110 · Thermal conductivity: typical, 20 °CCopper C110 · Thermal expansion: typical, mean 20-100 °CCopper C110 · Specific heat: typical, 20 °CCopper C110 · Melting point: solidus-liquidus
  2. 2
    Delrin Acetal Resin Design Guide, Module IIIDuPontarchived copyPlastic POM/Acetal · Yield strength: typical (single ASTM D638 tensile strength)Plastic POM/Acetal · Ultimate tensile strength: typicalPlastic POM/Acetal · Compressive strength: compressive stress at 10% deformationPlastic POM/Acetal · Flexural strength: flexural yield strength, typicalPlastic POM/Acetal · Elongation at break: typicalPlastic POM/Acetal · Young's modulus (stiffness): typicalPlastic POM/Acetal · Poisson's ratio: typicalPlastic POM/Acetal · Thermal conductivity: typicalPlastic POM/Acetal · Thermal expansion: mean, 29 to 60 °CPlastic POM/Acetal · Specific heat: average -18 to 100 °C, Delrin acetal resins (not grade-specific)Plastic POM/Acetal · Melting point: crystalline melting pointPlastic POM/Acetal · Max service temperature: HDT 1.8 MPa (annealed)
  3. 3
    Delrin 100 Product Data SheetDuPontPlastic POM/Acetal · Density: typical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
  4. 4
    Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Copper C110 stronger than Plastic POM/Acetal?

Copper C110 is stronger: its yield strength is 69 MPa against 69 MPa for Plastic POM/Acetal (0%).

Which is lighter, Copper C110 or Plastic POM/Acetal?

Plastic POM/Acetal is lighter: 1,420 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or Plastic POM/Acetal?

Copper C110 is stiffer: Young's modulus 117 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Copper C110 deflects less under the same load.

Which is lighter for the same job, Copper C110 or Plastic POM/Acetal?

For the same stiffness or strength: Copper C110 is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic POM/Acetal is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110Plastic POM/Acetal
Stiff rod or tie (tension)lighter6.67x heavier
Stiff beam (bending)lighter3% heavier
Stiff panel or plate1.81x heavierlighter
Strong rod or tie6.28x heavierlighter
Strong beam6.28x heavierlighter
Strong panel or plate6.28x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C110 or Plastic POM/Acetal?

Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 55% for Copper C110.

Thermal

Which conducts heat better, Copper C110 or Plastic POM/Acetal?

Copper C110 conducts heat better: 391 W/m·K against 0.4 W/m·K for Plastic POM/Acetal.

Which expands less with temperature?

Copper C110 expands less: 16.9 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.

Related comparisons