Materials / Compare

Copper C110 vs. Stainless Steel 316

Compare Copper C110 vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Change either side
Copper C110Wrought
Stainless Steel 316Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength69MPasourcetypical, 0.5% extension under load265MPasourcetypical (representative), annealed 1.0 mm sheet
Ultimate tensile strength221MPasourcetypical583MPasourcetypical (representative), annealed 1.0 mm sheet
Elongation at break55%sourcetypical, 1 in. rod61%sourcetypical (representative), annealed, in 2 in. (51 mm)
Young's modulus (stiffness)117GPasourcetypical200GPasourcetypical, in tension
Density8,913kg/m³sourcenominal8,027kg/m³sourcetypical
Strength to weight7.74kN·m/kg33kN·m/kg4.26x higher
Stiffness to weight13.1MN·m/kg24.9MN·m/kg1.89x higher
Poisson's ratio0.34sourcereference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)0.3sourcedesign value (structural stainless steels)
Shear modulus43.7GPa76.9GPa1.76x stiffer in shear
Bulk modulus122GPa167GPa
Speed of sound3,626m/s4,992m/s
Thermal
Thermal conductivity391W/m·Ksourcetypical, 20 °C14.6W/m·Ksource20–100 °C
Thermal expansion16.9µm/m·Ksourcetypical, mean 20-100 °C16.5µm/m·Ksourcemean, 20–100 °C
100 mm part over a 50 °C swing84.5µm growth82.5µm growth2% less
Specific heat385J/kg·Ksourcetypical, 20 °C450J/kg·Ksourceat 20 °C
Heats up and cools (diffusivity)114mm²/s28.2x faster4.04mm²/s
Thermal shock resistance8,992W/m11x more resistant821W/m
Melting point1,065–1,083°Csourcesolidus-liquidus1,390–1,440°Csourcemelting range
Max service temperaturenot sourced871–899°Csourceoxidation (scaling) limit in air
Values forC11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical valuesATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Copper C110 stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against 69 MPa for Copper C110 (3.84x).

Which is lighter, Copper C110 or Stainless Steel 316?

Stainless Steel 316 is lighter: 8,027 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 117 GPa for Copper C110, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Copper C110 or Stainless Steel 316?

For the same stiffness or strength: Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110Stainless Steel 316
Stiff rod or tie (tension)1.89x heavierlighter
Stiff beam (bending)45% heavierlighter
Stiff panel or plate33% heavierlighter
Strong rod or tie4.26x heavierlighter
Strong beam2.72x heavierlighter
Strong panel or plate2.18x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Copper C110 or Stainless Steel 316?

Copper C110 conducts heat better: 391 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 16.9 µm/m·K for Copper C110.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelCopper C110Stainless Steel 316
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickCopper C110Stainless Steel 316
Strength against density

Related comparisons