Materials / Compare

Copper C12200 vs. Stainless Steel 304

Compare Copper C12200 vs. Stainless Steel 304 strength, stiffness, weight and thermal properties.

Copper C12200Wrought
Stainless Steel 304Wrought
MechanicalCopper C12200Stainless Steel 304
Yield strength69MPa1241MPa23.49x stronger
Ultimate tensile strength221MPa1586MPa22.65x stronger
Elongation at break45%155%222% more ductile
Young's modulus (stiffness)117GPa1193GPa21.65x stiffer
Density8,941kg/m³18,030kg/m³211% lighter
Strength to weight7.72kN·m/kg30kN·m/kg3.89x higher
Stiffness to weight13.1MN·m/kg24MN·m/kg1.83x higher
Poisson's ratio0.343design value0.34
Shear modulus43.7GPa74.2GPa1.7x stiffer in shear
Bulk modulus122GPa161GPa32% higher
Speed of sound3,621m/s4,903m/s35% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 304
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 304
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C12200Stainless Steel 304
Thermal conductivity339W/m·K120.9x more heat through a finat 100 °C16.2W/m·K2
Thermal expansion16.9µm/m·K1mean16.9µm/m·K2
100 mm part over a 50 °C swing84.5µm growth84.5µm growth
Specific heat385J/kg·K1mean500J/kg·K230% higher
Heats up and cools (diffusivity)98.5mm²/s24.4x faster4.03mm²/s
Thermal shock resistance7,799W/m9.31x more resistant838W/m
Melting pointliquidus1,083°C1melting range1,399–1,454°C2
Max service temperaturenot sourcedcontinuous899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 304
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 304
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Copper Development Association, Cleveland-Cliffs, Wieland, Steel Construction Institute
Copper C12200
C12200 phosphorus-deoxidized copper (DHP, the air-conditioning and refrigeration tube copper), tube annealed to 0.050 mm grain size (OS050), 0.065 in. wall, copper.org typical values
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    C12200 Alloy (copper.org)Copper Development Associationarchived copyCopper C12200 · Yield strength: typical, 0.5% extension under load, 0.065 in. tubeCopper C12200 · Ultimate tensile strength: typical, 0.065 in. tubeCopper C12200 · Elongation at break: typical, 0.065 in. tubeCopper C12200 · Young's modulus (stiffness): typicalCopper C12200 · Density: nominalCopper C12200 · Thermal conductivity: typical, 20 °CCopper C12200 · Thermal expansion: typical, mean 20-100 °CCopper C12200 · Specific heat: typical, 20 °CCopper C12200 · Melting point: liquidus
  2. 2
    304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
  3. 3
    Wieland-K19 (Cu-DHP, C12200) Data SheetWielandarchived copyCopper C12200 · Poisson's ratio: reference value at room temperature (Wieland-K19 = Cu-DHP = C12200, rolled products)
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Copper C12200 stronger than Stainless Steel 304?

Stainless Steel 304 is stronger: its yield strength is 241 MPa against 69 MPa for Copper C12200 (3.49x).

Which is lighter, Copper C12200 or Stainless Steel 304?

Stainless Steel 304 is lighter: 8,030 kg/m³ against 8,941 kg/m³ for Copper C12200.

Which is stiffer, Copper C12200 or Stainless Steel 304?

Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 117 GPa for Copper C12200, so the same part in Stainless Steel 304 deflects less under the same load.

Which is lighter for the same job, Copper C12200 or Stainless Steel 304?

For the same stiffness or strength: Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C12200Stainless Steel 304
Stiff rod or tie (tension)1.83x heavierlighter
Stiff beam (bending)43% heavierlighter
Stiff panel or plate31% heavierlighter
Strong rod or tie3.89x heavierlighter
Strong beam2.56x heavierlighter
Strong panel or plate2.08x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C12200 or Stainless Steel 304?

Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 45% for Copper C12200.

Thermal

Which conducts heat better, Copper C12200 or Stainless Steel 304?

Copper C12200 conducts heat better: 339 W/m·K against 16.2 W/m·K for Stainless Steel 304.

Which expands less with temperature?

Copper C12200 expands less: 16.9 µm/m·K against 16.9 µm/m·K for Stainless Steel 304.