Materials / Compare

Copper C12200 vs. Stainless Steel 316

Compare Copper C12200 vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Copper C12200Wrought
Stainless Steel 316Wrought
MechanicalCopper C12200Stainless Steel 316
Yield strength69MPa1265MPa23.84x stronger
Ultimate tensile strength221MPa1583MPa22.64x stronger
Elongation at break45%161%236% more ductile
Young's modulus (stiffness)117GPa1200GPa21.71x stiffer
Density8,941kg/m³18,027kg/m³211% lighter
Strength to weight7.72kN·m/kg33kN·m/kg4.28x higher
Stiffness to weight13.1MN·m/kg24.9MN·m/kg1.9x higher
Poisson's ratio0.343design value0.34
Shear modulus43.7GPa76.9GPa1.76x stiffer in shear
Bulk modulus122GPa167GPa37% higher
Speed of sound3,621m/s4,992m/s38% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 316
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 316
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C12200Stainless Steel 316
Thermal conductivity339W/m·K123.2x more heat through a fin20–100 °C14.6W/m·K2
Thermal expansion16.9µm/m·K1mean16.5µm/m·K2
100 mm part over a 50 °C swing84.5µm growth82.5µm growth2% less
Specific heat385J/kg·K1at 20 °C450J/kg·K217% higher
Heats up and cools (diffusivity)98.5mm²/s24.4x faster4.04mm²/s
Thermal shock resistance7,799W/m9.5x more resistant821W/m
Melting pointliquidus1,083°C1melting range1,390–1,440°C2
Max service temperaturenot sourcedoxidation871–899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 316
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C12200Stainless Steel 316
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Copper Development Association, ATI, Wieland, Steel Construction Institute
Copper C12200
C12200 phosphorus-deoxidized copper (DHP, the air-conditioning and refrigeration tube copper), tube annealed to 0.050 mm grain size (OS050), 0.065 in. wall, copper.org typical values
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    C12200 Alloy (copper.org)Copper Development Associationarchived copyCopper C12200 · Yield strength: typical, 0.5% extension under load, 0.065 in. tubeCopper C12200 · Ultimate tensile strength: typical, 0.065 in. tubeCopper C12200 · Elongation at break: typical, 0.065 in. tubeCopper C12200 · Young's modulus (stiffness): typicalCopper C12200 · Density: nominalCopper C12200 · Thermal conductivity: typical, 20 °CCopper C12200 · Thermal expansion: typical, mean 20-100 °CCopper C12200 · Specific heat: typical, 20 °CCopper C12200 · Melting point: liquidus
  2. 2
    ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
  3. 3
    Wieland-K19 (Cu-DHP, C12200) Data SheetWielandarchived copyCopper C12200 · Poisson's ratio: reference value at room temperature (Wieland-K19 = Cu-DHP = C12200, rolled products)
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Copper C12200 stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against 69 MPa for Copper C12200 (3.84x).

Which is lighter, Copper C12200 or Stainless Steel 316?

Stainless Steel 316 is lighter: 8,027 kg/m³ against 8,941 kg/m³ for Copper C12200.

Which is stiffer, Copper C12200 or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 117 GPa for Copper C12200, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Copper C12200 or Stainless Steel 316?

For the same stiffness or strength: Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C12200Stainless Steel 316
Stiff rod or tie (tension)1.9x heavierlighter
Stiff beam (bending)46% heavierlighter
Stiff panel or plate33% heavierlighter
Strong rod or tie4.28x heavierlighter
Strong beam2.73x heavierlighter
Strong panel or plate2.18x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C12200 or Stainless Steel 316?

Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 45% for Copper C12200.

Thermal

Which conducts heat better, Copper C12200 or Stainless Steel 316?

Copper C12200 conducts heat better: 339 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 16.9 µm/m·K for Copper C12200.

Related comparisons