Materials / Compare
DMLS 316L Stainless Steel vs. Plastic Nylon PA66
Compare DMLS 316L Stainless Steel vs. Plastic Nylon PA66 strength, stiffness, weight and thermal properties.
| Mechanical | DMLS 316L Stainless Steel | Plastic Nylon PA66 |
|---|---|---|
| Yield strength | 530MPa16.24x stronger | 85MPa2 |
| Ultimate tensile strength | 640MPa1 | not stated (yield given) |
| Elongation at break | 40%133% more ductile | 30%2 |
| Young's modulus (stiffness) | 185GPa361.7x stiffer | 3GPa2 |
| Density | part density7,900kg/m³4 | 1,130kg/m³26.99x lighter |
| Strength to weight | 67.1kN·m/kg | 75.2kN·m/kg12% higher |
| Stiffness to weight | 23.4MN·m/kg8.82x higher | 2.65MN·m/kg |
| Poisson's ratio | base material0.35 | base material0.46 |
| Shear modulus | 71.2GPa66.4x stiffer in shear | 1.07GPa |
| Bulk modulus | 154GPa30.8x higher | 5GPa |
| Speed of sound | 4,839m/s2.97x faster | 1,629m/s |
| Thermal | DMLS 316L Stainless Steel | Plastic Nylon PA66 |
|---|---|---|
| Thermal conductivity | base material16.2W/m·K749.1x more heat through a fin | 0.33W/m·K2 |
| Thermal expansion | mean 25-100 °C15.7µm/m·K16.23x less | longitudinal98µm/m·K2 |
| 100 mm part over a 50 °C swing | 78.6µm growth6.23x less | 490µm growth |
| Specific heat | base material500J/kg·K7 | 1,700J/kg·K23.4x higher |
| Heats up and cools (diffusivity) | 4.1mm²/s23.9x faster | 0.172mm²/s |
| Thermal shock resistance | 2,067W/m36.1x more resistant | 57.2W/m |
| Melting point | not sourced | DSC260°C2 |
| Max service temperature | not sourced | 101°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: EOS GmbH, BASF, Steel Construction Institute, Covestro, Cleveland-Cliffs
- DMLS 316L Stainless Steel
- EOS StainlessSteel 316L (powder 9011-0032), EOS M 290, ParameterSet 316L 20µm Surface M290/400W, as manufactured, horizontal; ISO 6892-1
- Plastic Nylon PA66
- BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
- 1EOS StainlessSteel 316L Material Data SheetEOS GmbHarchived copyDMLS 316L Stainless Steel · Yield strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Ultimate tensile strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Elongation at break: typical at break, as manufactured, horizontalDMLS 316L Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Ultramid A3K Product InformationBASFPlastic Nylon PA66 · Yield strength: typical, dryPlastic Nylon PA66 · Elongation at break: nominal strain at break, dryPlastic Nylon PA66 · Young's modulus (stiffness): typical, dryPlastic Nylon PA66 · Density: typicalPlastic Nylon PA66 · Thermal conductivity: typicalPlastic Nylon PA66 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA66 · Specific heat: typicalPlastic Nylon PA66 · Melting point: DSCPlastic Nylon PA66 · Max service temperature: IEC 60216 temperature index, 20000 h
- 3EOS StainlessSteel 316L Material Data Sheet, M 280 and M 290 (2014)EOS GmbHarchived copyDMLS 316L Stainless Steel · Young's modulus (stiffness): typical, as built, horizontal (XY); EOSINT M280-400W / M290-400W, 316L_Surface 1.0, 20 µm (2014 sheet)
- 4EOS StainlessSteel 316L Material Data Sheet, FlexLine, M 290 (2016)EOS GmbHarchived copyDMLS 316L Stainless Steel · Density: part density (ISO 3369, not labelled min or typical), EOS M 290, 40 µm FlexLine
- 5Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyDMLS 316L Stainless Steel · Poisson's ratio: base material: austenitic stainless steels incl. 1.4404 (316L), design value
- 6Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
- 7316/316L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 316L Stainless Steel · Thermal conductivity: base material: wrought 316/316L (Cleveland-Cliffs), at 100 °CDMLS 316L Stainless Steel · Specific heat: base material: wrought 316/316L (Cleveland-Cliffs), 0-100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 316L Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS 316L Stainless Steel stronger than Plastic Nylon PA66?
DMLS 316L Stainless Steel is stronger: its yield strength is 530 MPa against 85 MPa for Plastic Nylon PA66 (6.24x).
Which is lighter, DMLS 316L Stainless Steel or Plastic Nylon PA66?
Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 7,900 kg/m³ for DMLS 316L Stainless Steel.
Which is stiffer, DMLS 316L Stainless Steel or Plastic Nylon PA66?
DMLS 316L Stainless Steel is stiffer: Young's modulus 185 GPa against 3 GPa for Plastic Nylon PA66, so the same part in DMLS 316L Stainless Steel deflects less under the same load.
Which is lighter for the same job, DMLS 316L Stainless Steel or Plastic Nylon PA66?
For the same stiffness or strength: DMLS 316L Stainless Steel is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic Nylon PA66 is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | DMLS 316L Stainless Steel | Plastic Nylon PA66 |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 8.82x heavier |
| Stiff beam (bending) | lighter | 12% heavier |
| Stiff panel or plate | 1.77x heavier | lighter |
| Strong rod or tie | 12% heavier | lighter |
| Strong beam | 2.06x heavier | lighter |
| Strong panel or plate | 2.8x heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS 316L Stainless Steel or Plastic Nylon PA66?
DMLS 316L Stainless Steel stretches further before it breaks: 40% elongation at break against 30% for Plastic Nylon PA66.
Thermal
Which conducts heat better, DMLS 316L Stainless Steel or Plastic Nylon PA66?
DMLS 316L Stainless Steel conducts heat better: 16.2 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.
Which expands less with temperature?
DMLS 316L Stainless Steel expands less: 15.7 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.
Related comparisons
- DMLS 316L Stainless Steel vs. Steel AISI 1045
- DMLS 316L Stainless Steel vs. Steel
- DMLS 316L Stainless Steel vs. Steel A992
- DMLS 316L Stainless Steel vs. Steel AISI 1018
- Plastic Nylon PA66 vs. Plastic PMMA
- Plastic Nylon PA66 vs. Plastic Nylon PA6
- Plastic Nylon PA66 vs. FDM PAHT-CF
- Plastic Nylon PA66 vs. Plastic POM/Acetal