Materials / Compare

DMLS AlSi10Mg Aluminum vs. Glass

Compare DMLS AlSi10Mg Aluminum vs. Glass strength, stiffness, weight and thermal properties.

DMLS AlSi10Mg Aluminum3D printed metal (DMLS)
GlassNatural
MechanicalDMLS AlSi10Mg AluminumGlass
Yield strength270MPa1none (brittle)
Ultimate tensile strength450MPa111x stronger41MPa2
Flexural strengthnot sourcedmean MOR41MPa2
Elongation at break10.2%1none (brittle)
Young's modulus (stiffness)72GPa372GPa2
Density2,670kg/m³42,500kg/m³2
Strength to weight101kN·m/kg6.17x higher16.4kN·m/kg
Stiffness to weight27MN·m/kg28.8MN·m/kg7% higher
Poisson's ratiobase material0.3350.222
Shear modulus27.1GPa29.5GPa9% stiffer in shear
Bulk modulus70.6GPa1.65x higher42.9GPa
Speed of sound5,193m/s5,367m/s3% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS AlSi10Mg AluminumGlass
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS AlSi10Mg AluminumGlass
Strength against densityHigher and further left: stronger for its weight
ThermalDMLS AlSi10Mg AluminumGlass
Thermal conductivity110W/m·K1117x more heat through a fin0.937W/m·K2
Thermal expansionmean 25-100 °C20µm/m·K18.3µm/m·K22.41x less
100 mm part over a 50 °C swing100µm growth41.5µm growth2.41x less
Specific heatbase material963J/kg·K5880J/kg·K2
Heats up and cools (diffusivity)42.8mm²/s100x faster0.426mm²/s
Thermal shock resistance13,819W/m276x more resistant50.1W/m
Max service temperaturenot sourcedstrain point511°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS AlSi10Mg AluminumGlass
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS AlSi10Mg AluminumGlass
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: EOS GmbH, Pilkington North America, Renishaw, U.S. Department of Defense
DMLS AlSi10Mg Aluminum
EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
  1. 1
    EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
  2. 2
    Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
  3. 3
    RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
  4. 4
    EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
  5. 5
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is DMLS AlSi10Mg Aluminum stronger than Glass?

DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against tensile strength 41 MPa for Glass (6.59x).

Which is lighter, DMLS AlSi10Mg Aluminum or Glass?

Glass is lighter: 2,500 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.

Which is stiffer, DMLS AlSi10Mg Aluminum or Glass?

DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 72 GPa for Glass, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.

Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Glass?

For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a strong rod or tie, strong beam, strong panel or plate; Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beDMLS AlSi10Mg AluminumGlass
Stiff rod or tie (tension)7% heavierlighter
Stiff beam (bending)7% heavierlighter
Stiff panel or plate7% heavierlighter
Strong rod or tielighter6.17x heavier
Strong beamlighter3.29x heavier
Strong panel or platelighter2.4x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, DMLS AlSi10Mg Aluminum or Glass?

DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.937 W/m·K for Glass.

Which expands less with temperature?

Glass expands less: 8.3 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.

Related comparisons