| Mechanical | DMLS AlSi10Mg Aluminum | Stainless Steel 303 |
|---|---|---|
| Yield strength | 270MPa1 | Outokumpu typical275MPa2 |
| Ultimate tensile strength | 450MPa1 | Outokumpu typical585MPa230% stronger |
| Elongation at break | 10.2%1 | Outokumpu typical35%23.43x more ductile |
| Young's modulus (stiffness) | 72GPa3 | at RT200GPa22.78x stiffer |
| Density | 2,670kg/m³42.96x lighter | at RT7,900kg/m³2 |
| Strength to weight | 101kN·m/kg2.91x higher | 34.8kN·m/kg |
| Stiffness to weight | 27MN·m/kg7% higher | 25.3MN·m/kg |
| Poisson's ratio | base material0.335 | design value0.36 |
| Shear modulus | 27.1GPa | 76.9GPa2.84x stiffer in shear |
| Bulk modulus | 70.6GPa | 167GPa2.36x higher |
| Speed of sound | 5,193m/s3% faster | 5,032m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Stainless Steel 303 |
|---|---|---|
| Thermal conductivity | 110W/m·K17.33x more heat through a fin | at RT15W/m·K2 |
| Thermal expansion | mean 25-100 °C20µm/m·K1 | mean16µm/m·K225% less |
| 100 mm part over a 50 °C swing | 100µm growth | 80µm growth25% less |
| Specific heat | base material963J/kg·K5 | at RT500J/kg·K2 |
| Heats up and cools (diffusivity) | 42.8mm²/s11.3x faster | 3.8mm²/s |
| Thermal shock resistance | 13,819W/m15.3x more resistant | 902W/m |
| Max service temperature | not sourced | continuous871°C7 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: EOS GmbH, Outokumpu, Renishaw, U.S. Department of Defense, Steel Construction Institute, Carpenter Technology
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Stainless Steel 303
- 1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
- 6Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
- 7Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (2%).
Which is lighter, DMLS AlSi10Mg Aluminum or Stainless Steel 303?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, DMLS AlSi10Mg Aluminum or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 72 GPa for DMLS AlSi10Mg Aluminum, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Stainless Steel 303?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | DMLS AlSi10Mg Aluminum | Stainless Steel 303 |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 7% heavier |
| Stiff beam (bending) | lighter | 1.78x heavier |
| Stiff panel or plate | lighter | 2.1x heavier |
| Strong rod or tie | lighter | 2.91x heavier |
| Strong beam | lighter | 2.92x heavier |
| Strong panel or plate | lighter | 2.93x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Stainless Steel 303?
Stainless Steel 303 stretches further before it breaks: 35% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Stainless Steel 303?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 15 W/m·K for Stainless Steel 303.
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Stainless Steel 303 vs. Stainless Steel 316
- Stainless Steel 303 vs. Stainless Steel 304
- Stainless Steel 303 vs. Steel AISI 1018
- Stainless Steel 303 vs. Steel