Materials / Compare

DMLS Ti-6Al-4V ELI Titanium vs. Zinc Zamak 3

Compare DMLS Ti-6Al-4V ELI Titanium vs. Zinc Zamak 3 strength, stiffness, weight and thermal properties.

DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Zinc Zamak 3Cast
MechanicalDMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Yield strength1,100MPa14.98x stronger221MPa2
Ultimate tensile strength1,270MPa14.49x stronger283MPa2
Elongation at break8.7%110%215% more ductile
Young's modulus (stiffness)same maker and process110GPa329% stiffer85.5GPa2
Density4,400kg/m³11.5x lighter6,600kg/m³2
Strength to weight250kN·m/kg7.47x higher33.5kN·m/kg
Stiffness to weight25MN·m/kg1.93x higher13MN·m/kg
Poisson's ratiowrought TIMETAL 6-40.34240.275
Shear modulus41GPa22% stiffer in shear33.7GPa
Bulk modulus116GPa1.87x higher62GPa
Speed of sound5,000m/s39% faster3,599m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Strength against densityHigher and further left: stronger for its weight
ThermalDMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Thermal conductivitybase material6.6W/m·K6113W/m·K217.1x more heat through a fin
Thermal expansionmean 25-100 °C9µm/m·K73.04x less27.4µm/m·K2
100 mm part over a 50 °C swing45µm growth3.04x less137µm growth
Specific heatbase material580J/kg·K639% higher419J/kg·K2
Heats up and cools (diffusivity)2.59mm²/s40.9mm²/s15.8x faster
Thermal shock resistance4,825W/m7,782W/m1.61x more resistant
Melting pointmelting range1,630–1,650°C4melting range381–387°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources7 documents: EOS GmbH, Nathan Trotter, TIMET, Eastern Alloys
DMLS Ti-6Al-4V ELI Titanium
EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14
Zinc Zamak 3
Zamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values
  1. 1
    EOS Titanium Ti64ELI Material Data Sheet, M 290 and M 400EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Yield strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Ultimate tensile strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Elongation at break: typical at break, as built (M400)DMLS Ti-6Al-4V ELI Titanium · Density: typical part density (ISO 3369), M400
  2. 2
    Zamak 3 Technical Data SheetNathan Trotterarchived copyZinc Zamak 3 · Yield strength: typicalZinc Zamak 3 · Ultimate tensile strength: typicalZinc Zamak 3 · Elongation at break: typical, in 2 in.Zinc Zamak 3 · Young's modulus (stiffness): typicalZinc Zamak 3 · Density: typicalZinc Zamak 3 · Thermal conductivity: typicalZinc Zamak 3 · Thermal expansion: typicalZinc Zamak 3 · Specific heat: typicalZinc Zamak 3 · Melting point: melting range
  3. 3
    EOS Titanium Ti64 Material Data Sheet, M 290 (2022)EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Young's modulus (stiffness): same maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
  4. 4
    TIMETAL 6-4 PropertiesTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Poisson's ratio: wrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measuredDMLS Ti-6Al-4V ELI Titanium · Melting point: melting range, wrought TIMETAL 6-4 (composition-level)
  5. 5
    Zinc Die Casting Properties Guide (2012)Eastern AlloysZinc Zamak 3 · Poisson's ratio: typical, Zamak 3 hot-chamber die cast
  6. 6
    TIMETAL 6-4 Data SheetTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal conductivity: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °CDMLS Ti-6Al-4V ELI Titanium · Specific heat: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
  7. 7
    EOS Titanium Ti64 Grade 23 Material Data SheetEOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal expansion: mean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is DMLS Ti-6Al-4V ELI Titanium stronger than Zinc Zamak 3?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 221 MPa for Zinc Zamak 3 (4.98x).

Which is lighter, DMLS Ti-6Al-4V ELI Titanium or Zinc Zamak 3?

DMLS Ti-6Al-4V ELI Titanium is lighter: 4,400 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which is stiffer, DMLS Ti-6Al-4V ELI Titanium or Zinc Zamak 3?

DMLS Ti-6Al-4V ELI Titanium is stiffer: Young's modulus 110 GPa against 85.5 GPa for Zinc Zamak 3, so the same part in DMLS Ti-6Al-4V ELI Titanium deflects less under the same load.

Which is lighter for the same job, DMLS Ti-6Al-4V ELI Titanium or Zinc Zamak 3?

For the same stiffness or strength: DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beDMLS Ti-6Al-4V ELI TitaniumZinc Zamak 3
Stiff rod or tie (tension)lighter1.93x heavier
Stiff beam (bending)lighter1.7x heavier
Stiff panel or platelighter1.63x heavier
Strong rod or tielighter7.47x heavier
Strong beamlighter4.37x heavier
Strong panel or platelighter3.35x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, DMLS Ti-6Al-4V ELI Titanium or Zinc Zamak 3?

Zinc Zamak 3 stretches further before it breaks: 10% elongation at break against 8.7% for DMLS Ti-6Al-4V ELI Titanium.

Thermal

Which conducts heat better, DMLS Ti-6Al-4V ELI Titanium or Zinc Zamak 3?

Zinc Zamak 3 conducts heat better: 113 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 27.4 µm/m·K for Zinc Zamak 3.

Related comparisons