Materials / Compare

Drywall vs. Magnesium AZ91D

Compare Drywall vs. Magnesium AZ91D strength, stiffness, weight and thermal properties.

DrywallNatural
Magnesium AZ91DCast
MechanicalDrywallMagnesium AZ91D
Yield strengthnot given (tensile used)150MPa1
Ultimate tensile strength1–2MPa2230MPa1
Compressive strength2.4MPa3not sourced
Elongation at breaknot sourced3%1
Young's modulus (stiffness)1–2GPa245GPa1
Densitynot sourced1,810kg/m³1
Strength to weightnot sourced82.9kN·m/kg
Stiffness to weightnot sourced24.9MN·m/kg
Poisson's rationot sourcedbase material0.354
Shear modulusnot sourced16.7GPa
Bulk modulusnot sourced50GPa
Speed of soundnot sourced4,986m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91D
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91D
Strength against densityHigher and further left: stronger for its weight
ThermalDrywallMagnesium AZ91D
Thermal conductivitynot sourced72W/m·K1
Thermal expansion16.7µm/m·K350% less25µm/m·K1
100 mm part over a 50 °C swing83.5µm growth50% less125µm growth
Specific heat1,090J/kg·K31,050J/kg·K1
Heats up and cools (diffusivity)not sourced37.9mm²/s
Thermal shock resistancenot sourced6,240W/m
Melting pointnot sourcedmelting range470–595°C1
Max service temperature52°C5not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91D
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91D
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Magnesium Elektron, USDA Forest Products Laboratory, Gypsum Association, U.S. Department of Defense, USG
Drywall
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
Magnesium AZ91D
ELEKTRON AZ91D magnesium die-casting alloy, as cast; Magnesium Elektron datasheet 475 (7/01), typical properties; Poisson from MIL-HDBK-5J for AZ91C castings.
  1. 1
    Elektron Die Casting Alloys (Datasheet 475)Magnesium Elektronarchived copyMagnesium AZ91D · Yield strength: typical, 0.2% tensile yield, ambient temperatureMagnesium AZ91D · Ultimate tensile strength: typical, ambient temperatureMagnesium AZ91D · Elongation at break: typical, ambient temperatureMagnesium AZ91D · Young's modulus (stiffness): typicalMagnesium AZ91D · Density: typicalMagnesium AZ91D · Thermal conductivity: typicalMagnesium AZ91D · Thermal expansion: typical, temperature range not statedMagnesium AZ91D · Specific heat: typicalMagnesium AZ91D · Melting point: melting range
  2. 2
    Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
  3. 3
    GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
  4. 4
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ91D · Poisson's ratio: base material: AZ91C casting (MIL-HDBK-5J handbook physical constant)
  5. 5
    Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Drywall stronger than Magnesium AZ91D?

Magnesium AZ91D is stronger: its yield strength is 150 MPa against tensile strength 1.5 MPa for Drywall (100x).

Which is stiffer, Drywall or Magnesium AZ91D?

Magnesium AZ91D is stiffer: Young's modulus 45 GPa against 1.5 GPa for Drywall, so the same part in Magnesium AZ91D deflects less under the same load.

Thermal

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 25 µm/m·K for Magnesium AZ91D.

Related comparisons