Materials / Compare

Drywall vs. Plastic UHMWPE

Compare Drywall vs. Plastic UHMWPE strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
Plastic UHMWPEBulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)20MPasourcetypical, tensile stress at yield ISO 527, 50 mm/min
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)43MPasourcetypical, tensile stress at break ISO 527, 50 mm/min
Compressive strength2.4MPasourcetypical, 70 F / 50% RHnot sourced
Elongation at breaknot sourced465%sourcetypical, nominal elongation at break ISO 527
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)0.66GPasourcetypical, tensile modulus ISO 527, 1 mm/min
Densitynot sourced930kg/m³sourcetypical
Strength to weightnot sourced21.5kN·m/kg
Stiffness to weightnot sourced0.71MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced842m/s
Thermal
Thermal conductivitynot sourced0.4W/m·Ksourcetypical, unfilled (narrative value, generic Celanese UHMWPE)
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C200µm/m·Ksourcetypical, 20 to 100 °C (generic Celanese UHMWPE)
100 mm part over a 50 °C swing83.5µm growth12x less1,000µm growth
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)not sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced130–138°CsourceDSC 10 K/min
Max service temperature52°Csourcemanufacturer sustained-exposure limit80°Csourcerecommended max constant operating temperature
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalCelanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Drywall stronger than Plastic UHMWPE?

Plastic UHMWPE is stronger: its yield strength is 20 MPa against tensile strength 1.5 MPa for Drywall (13.3x).

Which is stiffer, Drywall or Plastic UHMWPE?

Drywall is stiffer: Young's modulus 1.5 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Drywall deflects less under the same load.

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 200 µm/m·K for Plastic UHMWPE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic UHMWPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic UHMWPE
Strength against density

Related comparisons