Materials / Compare

FDM ASA vs. Plastic HDPE

Compare FDM ASA vs. Plastic HDPE strength, stiffness, weight and thermal properties.

Change either side
FDM ASA3D printed (FDM)
Plastic HDPEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 527
Ultimate tensile strength37MPasourcetypicalnot sourced
Flexural strength65MPasourcetypicalnot sourced
Elongation at break9.2%sourcetypicalnot sourced
Young's modulus (stiffness)2.45GPasourcetypical0.9GPasourcetypical, tensile modulus 23 °C ISO 527
Density1,050kg/m³sourcetypical950kg/m³sourcetypical, ISO 1183
Strength to weight35.2kN·m/kg39% higher25.3kN·m/kg
Stiffness to weight2.33MN·m/kg2.46x higher0.947MN·m/kg
Poisson's rationot sourced0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Shear modulusnot sourced0.316GPa
Bulk modulusnot sourced2GPa
Speed of sound1,528m/s973m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, typical0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, range120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
100 mm part over a 50 °C swing475µm growth26% less600µm growth
Specific heatnot sourced2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Heats up and cools (diffusivity)not sourced0.208mm²/s
Thermal shock resistancenot sourced56.9W/m
Max service temperature92°CsourceHDT 1.8 MPanot sourced
Values forBambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM ASA stronger than Plastic HDPE?

FDM ASA is stronger: its tensile strength is 37 MPa against yield strength 24 MPa for Plastic HDPE (1.54x).

Which is lighter, FDM ASA or Plastic HDPE?

Plastic HDPE is lighter: 950 kg/m³ against 1,050 kg/m³ for FDM ASA.

Which is stiffer, FDM ASA or Plastic HDPE?

FDM ASA is stiffer: Young's modulus 2.45 GPa against 0.9 GPa for Plastic HDPE, so the same part in FDM ASA deflects less under the same load.

Which is lighter for the same job, FDM ASA or Plastic HDPE?

For the same stiffness or strength: FDM ASA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM ASAPlastic HDPE
Stiff rod or tie (tension)lighter2.46x heavier
Stiff beam (bending)lighter49% heavier
Stiff panel or platelighter26% heavier
Strong rod or tielighter39% heavier
Strong beamlighter21% heavier
Strong panel or platelighter12% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, FDM ASA or Plastic HDPE?

Plastic HDPE conducts heat better: 0.445 W/m·K against 0.17 W/m·K for FDM ASA.

Which expands less with temperature?

FDM ASA expands less: 95 µm/m·K against 120 µm/m·K for Plastic HDPE.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASAPlastic HDPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASAPlastic HDPE
Strength against density

Related comparisons