Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength37MPasourcetypical80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strength65MPasourcetypical115MPasourcetypical1.77x stronger in bending
Elongation at break9.2%sourcetypical1.67x more ductile5.5%sourcetypical
Young's modulus (stiffness)2.45GPasourcetypical3.3GPasourcetypical, short-term
Density1,050kg/m³sourcetypical13% lighter1,190kg/m³sourcetypical
Strength to weight35.2kN·m/kg67.2kN·m/kg1.91x higher
Stiffness to weight2.33MN·m/kg2.77MN·m/kg19% higher
Poisson's rationot sourced0.37sourcetypical
Shear modulusnot sourced1.2GPa
Bulk modulusnot sourced4.23GPa
Speed of sound1,528m/s1,665m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, typical0.19W/m·Ksourcetypical
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, range70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing475µm growth350µm growth36% less
Specific heatnot sourced1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced0.109mm²/s
Thermal shock resistancenot sourced41.5W/m
Max service temperature92°CsourceHDT 1.8 MPa80°Csourcemax. permanent service temperature
Values forBambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM ASA stronger than Plastic PMMA?

Plastic PMMA is stronger: its tensile strength is 80 MPa against 37 MPa for FDM ASA (2.16x).

Which is lighter, FDM ASA or Plastic PMMA?

FDM ASA is lighter: 1,050 kg/m³ against 1,190 kg/m³ for Plastic PMMA.

Which is stiffer, FDM ASA or Plastic PMMA?

Plastic PMMA is stiffer: Young's modulus 3.3 GPa against 2.45 GPa for FDM ASA, so the same part in Plastic PMMA deflects less under the same load.

Which is lighter for the same job, FDM ASA or Plastic PMMA?

For the same stiffness or strength: FDM ASA is lighter for a stiff panel or plate; Plastic PMMA is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM ASAPlastic PMMA
Stiff rod or tie (tension)19% heavierlighter
Stiff beam (bending)2% heavierlighter
Stiff panel or platelighter3% heavier
Strong rod or tie1.91x heavierlighter
Strong beam48% heavierlighter
Strong panel or plate30% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM ASA or Plastic PMMA?

FDM ASA stretches further before it breaks: 9.2% elongation at break against 5.5% for Plastic PMMA.

Which conducts heat better, FDM ASA or Plastic PMMA?

Plastic PMMA conducts heat better: 0.19 W/m·K against 0.17 W/m·K for FDM ASA.

Which expands less with temperature?

Plastic PMMA expands less: 70 µm/m·K against 95 µm/m·K for FDM ASA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM ASAPlastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM ASAPlastic PMMA
Strength against density