Compare FDM ASA vs. Rubber strength, stiffness, weight and thermal properties.

Change either side
FDM ASA3D printed (FDM)
RubberBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength37MPasourcetypical1.61x stronger23MPasourcetypical
Flexural strength65MPasourcetypicalnot sourced
Elongation at break9.2%sourcetypical830%sourcetypical90.2x more ductile
Young's modulus (stiffness)2.45GPasourcetypicalnot sourced
Density1,050kg/m³sourcetypical960kg/m³sourcetypical (specific gravity)
Strength to weight35.2kN·m/kg47% higher24kN·m/kg
Stiffness to weight2.33MN·m/kgnot sourced
Poisson's rationot sourced0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,528m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, typical0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourced1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)not sourced0.0836mm²/s
Thermal shock resistancenot sourcednot sourced
Max service temperature92°CsourceHDT 1.8 MPa70°Csourcecontinuous use operating range
Values forBambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM ASA stronger than Rubber?

FDM ASA is stronger: its tensile strength is 37 MPa against 23 MPa for Rubber (1.61x).

Which is lighter, FDM ASA or Rubber?

Rubber is lighter: 960 kg/m³ against 1,050 kg/m³ for FDM ASA.

Which is lighter for the same job, FDM ASA or Rubber?

For the same stiffness or strength: FDM ASA is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM ASARubber
Strong rod or tielighter47% heavier
Strong beamlighter26% heavier
Strong panel or platelighter16% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM ASA or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 9.2% for FDM ASA.

Which conducts heat better, FDM ASA or Rubber?

FDM ASA conducts heat better: 0.17 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM ASA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM ASARubber
Strength against density