Materials / Compare

FDM ASA vs. SLA Resin Standard

Compare FDM ASA vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
FDM ASA3D printed (FDM)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength37MPasourcetypical60MPasourcetypical1.62x stronger
Flexural strength65MPasourcetypical105MPasourcetypical1.62x stronger in bending
Elongation at break9.2%sourcetypical15% more ductile8%sourcetypical
Young's modulus (stiffness)2.45GPasourcetypical2.75GPasourcetypical12% stiffer
Density1,050kg/m³sourcetypicalnot sourced
Strength to weight35.2kN·m/kgnot sourced
Stiffness to weight2.33MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,528m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, typicalnot sourced
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Luran S 777K injection-molding ASA, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Max service temperature92°CsourceHDT 1.8 MPa1.56x hotter59°CsourceHDT 1.8 MPa
Values forBambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA and SLA Resin Standard are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM ASA stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against 37 MPa for FDM ASA (1.62x).

Which is stiffer, FDM ASA or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 2.45 GPa for FDM ASA, so the same part in SLA Resin Standard deflects less under the same load.

Which is more ductile, FDM ASA or SLA Resin Standard?

FDM ASA stretches further before it breaks: 9.2% elongation at break against 8% for SLA Resin Standard.

Which handles higher temperatures, FDM ASA or SLA Resin Standard?

FDM ASA does: 92 °C against 59 °C for SLA Resin Standard, both HDT 1.8 MPa.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM ASA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM ASA
Strength against density

Related comparisons