Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
Plastic PLA
Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.
Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM HIPS and Plastic PLA are 3D printed: their properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is FDM HIPS stronger than Plastic PLA?
Plastic PLA is stronger: its yield strength is 52.5 MPa against tensile strength 18.4 MPa for FDM HIPS (2.85x).
Which is lighter, FDM HIPS or Plastic PLA?
FDM HIPS is lighter: 1,023 kg/m³ against 1,240 kg/m³ for Plastic PLA.
Which is stiffer, FDM HIPS or Plastic PLA?
Plastic PLA is stiffer: Young's modulus 3.25 GPa against 1.59 GPa for FDM HIPS, so the same part in Plastic PLA deflects less under the same load.
Which is lighter for the same job, FDM HIPS or Plastic PLA?
For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
FDM HIPS
Plastic PLA
Stiff rod or tie (tension)
1.69x heavier
lighter
Stiff beam (bending)
18% heavier
lighter
Stiff panel or plate
5% heavier
lighter
Strong rod or tie
2.35x heavier
lighter
Strong beam
1.66x heavier
lighter
Strong panel or plate
39% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, FDM HIPS or Plastic PLA?
Plastic PLA stretches further before it breaks: 7.8% elongation at break against 1.4% for FDM HIPS.
Thermal
Which conducts heat better, FDM HIPS or Plastic PLA?
FDM HIPS conducts heat better: 0.17 W/m·K against 0.13 W/m·K for Plastic PLA.