Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength92MPasourcetypical1.53x stronger60MPasourcetypical
Flexural strength125MPasourcetypical19% stronger in bending105MPasourcetypical
Elongation at break8.4%sourcetypical8%sourcetypical
Young's modulus (stiffness)3.86GPasourcetypical40% stiffer2.75GPasourcetypical
Density1,060kg/m³sourcetypicalnot sourced
Strength to weight86.8kN·m/kgnot sourced
Stiffness to weight3.64MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,908m/snot sourced
Thermal
Thermal conductivitynot sourcednot sourced
Thermal expansionnot sourcednot sourced
100 mm part over a 50 °C swingnot sourcednot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Melting point225°Csourcetypicalnot sourced
Glass transition70°Csourcetypicalnot sourced
Max service temperature170°CsourceHDT 1.8 MPa2.88x hotter59°CsourceHDT 1.8 MPa
Values forBambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM PAHT-CF and SLA Resin Standard are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM PAHT-CF stronger than SLA Resin Standard?

FDM PAHT-CF is stronger: its tensile strength is 92 MPa against 60 MPa for SLA Resin Standard (1.53x).

Which is stiffer, FDM PAHT-CF or SLA Resin Standard?

FDM PAHT-CF is stiffer: Young's modulus 3.86 GPa against 2.75 GPa for SLA Resin Standard, so the same part in FDM PAHT-CF deflects less under the same load.

Which handles higher temperatures, FDM PAHT-CF or SLA Resin Standard?

FDM PAHT-CF does: 170 °C against 59 °C for SLA Resin Standard, both HDT 1.8 MPa.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM PAHT-CF
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM PAHT-CF
Strength against density

Related comparisons