Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: ATI, Bambu Lab, Steel Construction Institute
FDM PAHT-CF
Bambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM PAHT-CF is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is FDM PAHT-CF stronger than Stainless Steel 316?
Stainless Steel 316 is stronger: its yield strength is 265 MPa against tensile strength 92 MPa for FDM PAHT-CF (2.88x).
Which is lighter, FDM PAHT-CF or Stainless Steel 316?
FDM PAHT-CF is lighter: 1,060 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, FDM PAHT-CF or Stainless Steel 316?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 3.86 GPa for FDM PAHT-CF, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, FDM PAHT-CF or Stainless Steel 316?
For the same stiffness or strength: FDM PAHT-CF is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 316 is lighter for a stiff rod or tie (tension).
Part that must be
FDM PAHT-CF
Stainless Steel 316
Stiff rod or tie (tension)
6.84x heavier
lighter
Stiff beam (bending)
lighter
5% heavier
Stiff panel or plate
lighter
2.03x heavier
Strong rod or tie
lighter
2.63x heavier
Strong beam
lighter
3.74x heavier
Strong panel or plate
lighter
4.46x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, FDM PAHT-CF or Stainless Steel 316?
Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 8.4% for FDM PAHT-CF.