Materials / Compare

Glass vs. Plastic Nylon

Compare Glass vs. Plastic Nylon strength, stiffness, weight and thermal properties.

GlassNatural
Plastic Nylon3D printed (FDM)
MechanicalGlassPlastic Nylon
Yield strengthnone (brittle)63.1MPa1
Ultimate tensile strength41MPa263.1MPa11.54x stronger
Flexural strengthmean MOR41MPa282.9MPa12.02x stronger in bending
Elongation at breaknone (brittle)not sourced
Young's modulus (stiffness)72GPa230.9x stiffer2.33GPa1
Density2,500kg/m³21,140kg/m³12.19x lighter
Strength to weight16.4kN·m/kg55.4kN·m/kg3.38x higher
Stiffness to weight28.8MN·m/kg14.1x higher2.04MN·m/kg
Poisson's ratio0.222base material0.43
Shear modulus29.5GPa35.4x stiffer in shear0.833GPa
Bulk modulus42.9GPa11x higher3.89GPa
Speed of sound5,367m/s3.75x faster1,430m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassPlastic Nylon
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassPlastic Nylon
Strength against densityHigher and further left: stronger for its weight
ThermalGlassPlastic Nylon
Thermal conductivity0.937W/m·K22.84x more heat through a finbase material0.33W/m·K4
Thermal expansion8.3µm/m·K2base material98–102µm/m·K4
100 mm part over a 50 °C swing41.5µm growth12x less500µm growth
Specific heat880J/kg·K2base material1,700J/kg·K41.93x higher
Heats up and cools (diffusivity)0.426mm²/s2.5x faster0.17mm²/s
Thermal shock resistance50.1W/m53.6W/m7% more resistant
Melting pointnot sourced188°C1
Glass transitionnot sourced55.1°C1
Max service temperaturestrain point511°C2HDT 0.455 MPa89.2°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassPlastic Nylon
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassPlastic Nylon
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: UltiMaker, Pilkington North America, Covestro, BASF
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
  1. 1
    Ultimaker Nylon Technical Data Sheet, v5.00UltiMakerarchived copyPlastic Nylon · Yield strength: typicalPlastic Nylon · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic Nylon · Flexural strength: typicalPlastic Nylon · Young's modulus (stiffness): typicalPlastic Nylon · Density: typicalPlastic Nylon · Melting point: typicalPlastic Nylon · Glass transition: typicalPlastic Nylon · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  4. 4
    Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Glass stronger than Plastic Nylon?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against tensile strength 41 MPa for Glass (1.54x).

Which is lighter, Glass or Plastic Nylon?

Plastic Nylon is lighter: 1,140 kg/m³ against 2,500 kg/m³ for Glass.

Which is stiffer, Glass or Plastic Nylon?

Glass is stiffer: Young's modulus 72 GPa against 2.33 GPa for Plastic Nylon, so the same part in Glass deflects less under the same load.

Which is lighter for the same job, Glass or Plastic Nylon?

For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic Nylon is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beGlassPlastic Nylon
Stiff rod or tie (tension)lighter14.1x heavier
Stiff beam (bending)lighter2.53x heavier
Stiff panel or platelighter43% heavier
Strong rod or tie3.38x heavierlighter
Strong beam2.92x heavierlighter
Strong panel or plate2.72x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Glass or Plastic Nylon?

Glass conducts heat better: 0.937 W/m·K against 0.33 W/m·K for Plastic Nylon.

Which expands less with temperature?

Glass expands less: 8.3 µm/m·K against 100 µm/m·K for Plastic Nylon.

Related comparisons