Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources4 documents: Victrex, Pilkington North America
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
1
VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
2
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
3
VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
4
VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Glass stronger than Plastic PEEK?
Plastic PEEK is stronger: its yield strength is 98 MPa against tensile strength 41 MPa for Glass (2.39x).
Which is lighter, Glass or Plastic PEEK?
Plastic PEEK is lighter: 1,300 kg/m³ against 2,500 kg/m³ for Glass.
Which is stiffer, Glass or Plastic PEEK?
Glass is stiffer: Young's modulus 72 GPa against 4 GPa for Plastic PEEK, so the same part in Glass deflects less under the same load.
Which is lighter for the same job, Glass or Plastic PEEK?
For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic PEEK is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Glass
Plastic PEEK
Stiff rod or tie (tension)
lighter
9.36x heavier
Stiff beam (bending)
lighter
2.21x heavier
Stiff panel or plate
lighter
36% heavier
Strong rod or tie
4.6x heavier
lighter
Strong beam
3.44x heavier
lighter
Strong panel or plate
2.97x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which handles higher temperatures, Glass or Plastic PEEK?
Glass does: 511 °C against 240 °C for Plastic PEEK.
Which conducts heat better, Glass or Plastic PEEK?
Glass conducts heat better: 0.937 W/m·K against 0.29 W/m·K for Plastic PEEK.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 55 µm/m·K for Plastic PEEK.