Materials / Compare

Iron vs. Plastic PEEK

Compare Iron vs. Plastic PEEK strength, stiffness, weight and thermal properties.

IronWrought
Plastic PEEKBulk polymer (molded or machined)
MechanicalIronPlastic PEEK
Yield strength186MPa11.9x stronger98MPa2
Ultimate tensile strength290MPa1not stated (yield given)
Compressive strengthnot sourced125MPa2
Flexural strengthnot sourced165MPa2
Elongation at break38%11.52x more ductile25%2
Young's modulus (stiffness)207GPa151.8x stiffer4GPa2
Density7,860kg/m³11,300kg/m³26.05x lighter
Strength to weight23.7kN·m/kg75.4kN·m/kg3.19x higher
Stiffness to weight26.3MN·m/kg8.56x higher3.08MN·m/kg
Poisson's ratio0.28230.384
Shear modulus80.7GPa55.7x stiffer in shear1.45GPa
Bulk modulus158GPa28.5x higher5.56GPa
Speed of sound5,132m/s2.93x faster1,754m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PEEK
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PEEK
Strength against densityHigher and further left: stronger for its weight
ThermalIronPlastic PEEK
Thermal conductivity73.2W/m·K1252x more heat through a fin0.29W/m·K2
Thermal expansionmean13.7µm/m·K14.01x less55µm/m·K2
100 mm part over a 50 °C swing68.5µm growth4.01x less275µm growth
Specific heat450J/kg·K12,200J/kg·K54.89x higher
Heats up and cools (diffusivity)20.7mm²/s204x faster0.101mm²/s
Thermal shock resistance3,447W/m43x more resistant80.1W/m
Melting point1,532°C11,189 °C higher343°C2
Glass transitionnot sourcedonset143°C2
Max service temperaturenot sourcedUL 746B RTI240°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PEEK
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PEEK
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Cleveland-Cliffs, Victrex, National Institute of Standards and Technology
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
  1. 1
    ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
  2. 2
    VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
  3. 3
    Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
  4. 4
    VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
  5. 5
    VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Iron stronger than Plastic PEEK?

Iron is stronger: its yield strength is 186 MPa against 98 MPa for Plastic PEEK (1.9x).

Which is lighter, Iron or Plastic PEEK?

Plastic PEEK is lighter: 1,300 kg/m³ against 7,860 kg/m³ for Iron.

Which is stiffer, Iron or Plastic PEEK?

Iron is stiffer: Young's modulus 207 GPa against 4 GPa for Plastic PEEK, so the same part in Iron deflects less under the same load.

Which is lighter for the same job, Iron or Plastic PEEK?

For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic PEEK is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beIronPlastic PEEK
Stiff rod or tie (tension)lighter8.56x heavier
Stiff beam (bending)lighter19% heavier
Stiff panel or plate1.62x heavierlighter
Strong rod or tie3.19x heavierlighter
Strong beam3.94x heavierlighter
Strong panel or plate4.39x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Iron or Plastic PEEK?

Iron stretches further before it breaks: 38% elongation at break against 25% for Plastic PEEK.

Thermal

Which conducts heat better, Iron or Plastic PEEK?

Iron conducts heat better: 73.2 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

Iron expands less: 13.7 µm/m·K against 55 µm/m·K for Plastic PEEK.