Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
5
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
6
S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Steel A992?
Steel A992 is stronger: its yield strength is 385 MPa against 220 MPa for Magnesium AZ31B-H24 (1.75x).
Which is lighter, Magnesium AZ31B-H24 or Steel A992?
Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 7,850 kg/m³ for Steel A992.
Which is stiffer, Magnesium AZ31B-H24 or Steel A992?
Steel A992 is stiffer: Young's modulus 200 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Steel A992 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Steel A992?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
Steel A992
Stiff rod or tie (tension)
about equal
about equal
Stiff beam (bending)
lighter
2.1x heavier
Stiff panel or plate
lighter
2.69x heavier
Strong rod or tie
lighter
2.54x heavier
Strong beam
lighter
3.06x heavier
Strong panel or plate
lighter
3.35x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Magnesium AZ31B-H24 or Steel A992?
Steel A992 stretches further before it breaks: 24.2% elongation at break against 13% for Magnesium AZ31B-H24.
Thermal
Which conducts heat better, Magnesium AZ31B-H24 or Steel A992?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 48 W/m·K for Steel A992.
Which expands less with temperature?
Steel A992 expands less: 12 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.