Materials / Compare

Magnesium AZ91D vs. Steel A992

Compare Magnesium AZ91D vs. Steel A992 strength, stiffness, weight and thermal properties.

Magnesium AZ91DCast
Steel A992Wrought
MechanicalMagnesium AZ91DSteel A992
Yield strength150MPa1385MPa22.57x stronger
Ultimate tensile strength230MPa1505MPa22.2x stronger
Elongation at break3%124.2%28.07x more ductile
Young's modulus (stiffness)45GPa1design value200GPa3
Density1,810kg/m³14.34x lighter7,850kg/m³4
Strength to weight82.9kN·m/kg1.69x higher49kN·m/kg
Stiffness to weight24.9MN·m/kg25.5MN·m/kg2% higher
Poisson's ratiobase material0.355design value0.33
Shear modulus16.7GPa76.9GPa4.62x stiffer in shear
Bulk modulus50GPa167GPa3.33x higher
Speed of sound4,986m/s5,048m/s1% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91DSteel A992
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91DSteel A992
Strength against densityHigher and further left: stronger for its weight
ThermalMagnesium AZ91DSteel A992
Thermal conductivity72W/m·K11.5x more heat through a fin48W/m·K4
Thermal expansion25µm/m·K112µm/m·K42.08x less
100 mm part over a 50 °C swing125µm growth60µm growth2.08x less
Specific heat1,050J/kg·K1base material460–480J/kg·K6
Heats up and cools (diffusivity)37.9mm²/s2.91x faster13mm²/s
Thermal shock resistance6,240W/m16% more resistant5,390W/m
Melting pointmelting range470–595°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91DSteel A992
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Solder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ91DSteel A992
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: Magnesium Elektron, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), U.S. Department of Defense, Ovako
Magnesium AZ91D
ELEKTRON AZ91D magnesium die-casting alloy, as cast; Magnesium Elektron datasheet 475 (7/01), typical properties; Poisson from MIL-HDBK-5J for AZ91C castings.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
  1. 1
    Elektron Die Casting Alloys (Datasheet 475)Magnesium Elektronarchived copyMagnesium AZ91D · Yield strength: typical, 0.2% tensile yield, ambient temperatureMagnesium AZ91D · Ultimate tensile strength: typical, ambient temperatureMagnesium AZ91D · Elongation at break: typical, ambient temperatureMagnesium AZ91D · Young's modulus (stiffness): typicalMagnesium AZ91D · Density: typicalMagnesium AZ91D · Thermal conductivity: typicalMagnesium AZ91D · Thermal expansion: typical, temperature range not statedMagnesium AZ91D · Specific heat: typicalMagnesium AZ91D · Melting point: melting range
  2. 2
    Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
  3. 3
    ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
  4. 4
    Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
  5. 5
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ91D · Poisson's ratio: base material: AZ91C casting (MIL-HDBK-5J handbook physical constant)
  6. 6
    S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Magnesium AZ91D stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against 150 MPa for Magnesium AZ91D (2.57x).

Which is lighter, Magnesium AZ91D or Steel A992?

Magnesium AZ91D is lighter: 1,810 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Magnesium AZ91D or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 45 GPa for Magnesium AZ91D, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Magnesium AZ91D or Steel A992?

For the same stiffness or strength: Magnesium AZ91D is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel A992 is lighter for a stiff rod or tie (tension).

Part that must beMagnesium AZ91DSteel A992
Stiff rod or tie (tension)2% heavierlighter
Stiff beam (bending)lighter2.06x heavier
Stiff panel or platelighter2.64x heavier
Strong rod or tielighter1.69x heavier
Strong beamlighter2.31x heavier
Strong panel or platelighter2.71x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Magnesium AZ91D or Steel A992?

Steel A992 stretches further before it breaks: 24.2% elongation at break against 3% for Magnesium AZ91D.

Thermal

Which conducts heat better, Magnesium AZ91D or Steel A992?

Magnesium AZ91D conducts heat better: 72 W/m·K against 48 W/m·K for Steel A992.

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 25 µm/m·K for Magnesium AZ91D.