Materials / Compare
PCB Laminate FR-4 vs. SLA Resin Standard
Compare PCB Laminate FR-4 vs. SLA Resin Standard strength, stiffness, weight and thermal properties.
| Mechanical | PCB Laminate FR-4 | SLA Resin Standard |
|---|---|---|
| Yield strength | not given (tensile used) | not given (tensile used) |
| Ultimate tensile strength | 246–385MPa1 | 60MPa2 |
| Flexural strength | 531–621MPa1 | 105MPa2 |
| Elongation at break | not sourced | 8%2 |
| Young's modulus (stiffness) | 21.9–25.8GPa1 | 2.75GPa2 |
| Density | 1,920kg/m³3 | 1,210kg/m³41.59x lighter |
| Strength to weight | 164kN·m/kg3.31x higher | 49.6kN·m/kg |
| Stiffness to weight | 12.4MN·m/kg5.47x higher | 2.27MN·m/kg |
| Poisson's ratio | 0.171–0.1771 | not sourced |
| Shear modulus | 10.2GPa | not sourced |
| Bulk modulus | 12.2GPa | not sourced |
| Speed of sound | 3,525m/s2.34x faster | 1,508m/s |
| Thermal | PCB Laminate FR-4 | SLA Resin Standard |
|---|---|---|
| Thermal conductivity | 0.4W/m·K1 | 0.54W/m·K535% more heat through a fin |
| Thermal expansion | 13–14µm/m·K1 | mean -30 to 140 °C114µm/m·K5 |
| 100 mm part over a 50 °C swing | 67.5µm growth8.45x less | 571µm growth |
| Specific heat | 1,200–1,400J/kg·K3 | 1,800J/kg·K5 |
| Heats up and cools (diffusivity) | 0.16mm²/s | 0.248mm²/s1.55x faster |
| Thermal shock resistance | 324W/m | not sourced |
| Glass transition | 180°C1 | not sourced |
| Max service temperature | 130°C1 | HDT 1.8 MPa59°C2 |
| Try it on a partA sample part to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Isola, Formlabs, Park Electrochemical (Nelco)
- PCB Laminate FR-4
- Isola 370HR FR-4 laminate (Polyclad PCL-FR-370HR, 180 C Tg multifunctional epoxy, E-glass fabric), copper removed; Isola data sheet Revision C, last updated April 15, 2021. Woven-glass laminate: the sheet gives in-plane values per weave direction (length / cross) and the Z-axis CTE separately; the solver is isotropic per material.
- SLA Resin Standard
- Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
- 1370HR Laminate and Prepreg Data SheetIsolaarchived copyPCB Laminate FR-4 · Ultimate tensile strength: typical, in-plane: cross direction .. length direction (ASTM D3039)PCB Laminate FR-4 · Flexural strength: typical: cross direction .. length direction (IPC-TM-650 2.4.4B)PCB Laminate FR-4 · Young's modulus (stiffness): typical, in-plane: cross direction .. length direction (ASTM D790-15e2)PCB Laminate FR-4 · Poisson's ratio: typical, in-plane: cross direction .. length directionPCB Laminate FR-4 · Thermal conductivity: typical (ASTM E1952); direction not stated by the sheetPCB Laminate FR-4 · Thermal expansion: typical, in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)PCB Laminate FR-4 · Glass transition: typical, DSC (IPC-TM-650 2.4.25C)PCB Laminate FR-4 · Max service temperature: UL Relative Thermal Index (UL 796)
- 2Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
- 3N4000-6 Laminate Data Sheet (2006)Park Electrochemical (Nelco)archived copyPCB Laminate FR-4 · Density: typical, 50% resin content; another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HRPCB Laminate FR-4 · Specific heat: typical (ASTM E1461); another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HR
- 4Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
- 5Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is PCB Laminate FR-4 stronger than SLA Resin Standard?
PCB Laminate FR-4 is stronger: its tensile strength is 315 MPa against 60 MPa for SLA Resin Standard (5.26x).
Which is lighter, PCB Laminate FR-4 or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 1,920 kg/m³ for PCB Laminate FR-4.
Which is stiffer, PCB Laminate FR-4 or SLA Resin Standard?
PCB Laminate FR-4 is stiffer: Young's modulus 23.9 GPa against 2.75 GPa for SLA Resin Standard, so the same part in PCB Laminate FR-4 deflects less under the same load.
Which is lighter for the same job, PCB Laminate FR-4 or SLA Resin Standard?
For the same stiffness or strength: PCB Laminate FR-4 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | PCB Laminate FR-4 | SLA Resin Standard |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 5.47x heavier |
| Stiff beam (bending) | lighter | 1.86x heavier |
| Stiff panel or plate | lighter | 29% heavier |
| Strong rod or tie | lighter | 3.31x heavier |
| Strong beam | lighter | 1.91x heavier |
| Strong panel or plate | lighter | 44% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, PCB Laminate FR-4 or SLA Resin Standard?
SLA Resin Standard conducts heat better: 0.54 W/m·K against 0.4 W/m·K for PCB Laminate FR-4.
Which expands less with temperature?
PCB Laminate FR-4 expands less: 13.5 µm/m·K against 114 µm/m·K for SLA Resin Standard.
Related comparisons
- PCB Laminate FR-4 vs. PCB Board FR-4, 2 copper planes
- PCB Laminate FR-4 vs. Concrete
- PCB Laminate FR-4 vs. Plastic PPS GF40
- PCB Laminate FR-4 vs. Magnesium AZ31B-H24
- SLA Resin Standard vs. Plastic Polycarbonate
- SLA Resin Standard vs. Plastic Nylon
- SLA Resin Standard vs. FDM Polycarbonate
- SLA Resin Standard vs. Plastic POM/Acetal