Materials / Compare

Plastic ABS (bulk/injection) vs. Plastic HDPE

Compare Plastic ABS (bulk/injection) vs. Plastic HDPE strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
Plastic HDPEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °C24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 527
Ultimate tensile strengthnot sourcednot sourced
Flexural strength65MPasourcetypical, 23 °Cnot sourced
Elongation at break10%sourcenominal strain at break, 23 °Cnot sourced
Young's modulus (stiffness)2.3GPasourcetypical0.9GPasourcetypical, tensile modulus 23 °C ISO 527
Density1,040kg/m³sourcetypical950kg/m³sourcetypical, ISO 1183
Strength to weight43.3kN·m/kg1.71x higher25.3kN·m/kg
Stiffness to weight2.21MN·m/kg2.33x higher0.947MN·m/kg
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Shear modulus0.827GPa2.62x stiffer in shear0.316GPa
Bulk modulus3.48GPa2GPa
Speed of sound1,487m/s973m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypical0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Thermal expansion80–110µm/m·Ksourcerange120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
100 mm part over a 50 °C swing475µm growth26% less600µm growth
Specific heatnot sourced2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Heats up and cools (diffusivity)not sourced0.208mm²/s
Thermal shock resistance21.4W/m56.9W/m2.66x more resistant
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)not sourced
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic ABS (bulk/injection) stronger than Plastic HDPE?

Plastic ABS (bulk/injection) is stronger: its yield strength is 45 MPa against 24 MPa for Plastic HDPE (1.88x).

Which is lighter, Plastic ABS (bulk/injection) or Plastic HDPE?

Plastic HDPE is lighter: 950 kg/m³ against 1,040 kg/m³ for Plastic ABS (bulk/injection).

Which is stiffer, Plastic ABS (bulk/injection) or Plastic HDPE?

Plastic ABS (bulk/injection) is stiffer: Young's modulus 2.3 GPa against 0.9 GPa for Plastic HDPE, so the same part in Plastic ABS (bulk/injection) deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Plastic HDPE?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)Plastic HDPE
Stiff rod or tie (tension)lighter2.33x heavier
Stiff beam (bending)lighter46% heavier
Stiff panel or platelighter25% heavier
Strong rod or tielighter1.71x heavier
Strong beamlighter39% heavier
Strong panel or platelighter25% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS (bulk/injection) or Plastic HDPE?

Plastic HDPE conducts heat better: 0.445 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Plastic ABS (bulk/injection) expands less: 95 µm/m·K against 120 µm/m·K for Plastic HDPE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)Plastic HDPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)Plastic HDPE
Strength against density

Related comparisons