Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °Cnot given (tensile used)
Ultimate tensile strengthnot sourced80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strength65MPasourcetypical, 23 °C115MPasourcetypical
Elongation at break10%sourcenominal strain at break, 23 °C5.5%sourcetypical
Young's modulus (stiffness)2.3GPasourcetypical3.3GPasourcetypical, short-term
Density1,040kg/m³sourcetypical14% lighter1,190kg/m³sourcetypical
Strength to weight43.3kN·m/kg67.2kN·m/kg1.55x higher
Stiffness to weight2.21MN·m/kg2.77MN·m/kg25% higher
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)0.37sourcetypical
Shear modulus0.827GPa1.2GPa46% stiffer in shear
Bulk modulus3.48GPa4.23GPa
Speed of sound1,487m/s1,665m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypical0.19W/m·Ksourcetypical12% more heat through a fin
Thermal expansion80–110µm/m·Ksourcerange70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing475µm growth350µm growth36% less
Specific heatnot sourced1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced0.109mm²/s
Thermal shock resistance21.4W/m41.5W/m1.94x more resistant
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)80°Csourcemax. permanent service temperature
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic ABS (bulk/injection) stronger than Plastic PMMA?

Plastic PMMA is stronger: its tensile strength is 80 MPa against yield strength 45 MPa for Plastic ABS (bulk/injection) (1.78x).

Which is lighter, Plastic ABS (bulk/injection) or Plastic PMMA?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 1,190 kg/m³ for Plastic PMMA.

Which is stiffer, Plastic ABS (bulk/injection) or Plastic PMMA?

Plastic PMMA is stiffer: Young's modulus 3.3 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Plastic PMMA deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Plastic PMMA?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate; Plastic PMMA is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)Plastic PMMA
Stiff rod or tie (tension)25% heavierlighter
Stiff beam (bending)5% heavierlighter
Stiff panel or platelighter1% heavier
Strong rod or tie1.55x heavierlighter
Strong beam28% heavierlighter
Strong panel or plate17% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS (bulk/injection) or Plastic PMMA?

Plastic PMMA conducts heat better: 0.19 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Plastic PMMA expands less: 70 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)Plastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)Plastic PMMA
Strength against density

Related comparisons