Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °Cnot given (tensile used)
Ultimate tensile strengthnot sourced60MPasourcetypical
Flexural strength65MPasourcetypical, 23 °C105MPasourcetypical
Elongation at break10%sourcenominal strain at break, 23 °C8%sourcetypical
Young's modulus (stiffness)2.3GPasourcetypical2.75GPasourcetypical20% stiffer
Density1,040kg/m³sourcetypicalnot sourced
Strength to weight43.3kN·m/kgnot sourced
Stiffness to weight2.21MN·m/kgnot sourced
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.827GPanot sourced
Bulk modulus3.48GPanot sourced
Speed of sound1,487m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcetypicalnot sourced
Thermal expansion80–110µm/m·Ksourcerangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.4W/mnot sourced
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)59°CsourceHDT 1.8 MPa
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS (bulk/injection) stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against yield strength 45 MPa for Plastic ABS (bulk/injection) (33%).

Which is stiffer, Plastic ABS (bulk/injection) or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in SLA Resin Standard deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)
Strength against density

Related comparisons