Materials / Compare

Plastic ABS (bulk/injection) vs. Stainless Steel 316

Compare Plastic ABS (bulk/injection) vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
Stainless Steel 316Wrought
MechanicalPlastic ABS (bulk/injection)Stainless Steel 316
Yield strength45MPa1265MPa25.89x stronger
Ultimate tensile strengthnot stated (yield given)583MPa2
Flexural strength65MPa1not sourced
Elongation at break10%161%26.1x more ductile
Young's modulus (stiffness)2.3GPa1200GPa287x stiffer
Density1,040kg/m³17.72x lighter8,027kg/m³2
Strength to weight43.3kN·m/kg31% higher33kN·m/kg
Stiffness to weight2.21MN·m/kg24.9MN·m/kg11.3x higher
Poisson's ratio0.393design value0.34
Shear modulus0.827GPa76.9GPa93x stiffer in shear
Bulk modulus3.48GPa167GPa47.8x higher
Speed of sound1,487m/s4,992m/s3.36x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Stainless Steel 316
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Stainless Steel 316
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic ABS (bulk/injection)Stainless Steel 316
Thermal conductivity0.17W/m·K120–100 °C14.6W/m·K285.9x more heat through a fin
Thermal expansionrange80–110µm/m·K1mean16.5µm/m·K2
100 mm part over a 50 °C swing475µm growth82.5µm growth5.76x less
Specific heatnot sourcedat 20 °C450J/kg·K2
Heats up and cools (diffusivity)not sourced4.04mm²/s
Thermal shock resistance21.4W/m821W/m38.4x more resistant
Melting pointnot sourcedmelting range1,390–1,440°C2
Max service temperatureHDT 1.8 MPa94°C1oxidation871–899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Stainless Steel 316
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Stainless Steel 316
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: INEOS Styrolution, ATI, Covestro, Steel Construction Institute
Plastic ABS (bulk/injection)
INEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS (bulk/injection) · Yield strength: typical, tensile stress at yield 23 °CPlastic ABS (bulk/injection) · Flexural strength: typical, 23 °CPlastic ABS (bulk/injection) · Elongation at break: nominal strain at break, 23 °CPlastic ABS (bulk/injection) · Young's modulus (stiffness): typicalPlastic ABS (bulk/injection) · Density: typicalPlastic ABS (bulk/injection) · Thermal conductivity: typicalPlastic ABS (bulk/injection) · Thermal expansion: rangePlastic ABS (bulk/injection) · Max service temperature: HDT 1.8 MPa (annealed 4 h/80 °C)
  2. 2
    ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS (bulk/injection) · Poisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic ABS (bulk/injection) stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against 45 MPa for Plastic ABS (bulk/injection) (5.89x).

Which is lighter, Plastic ABS (bulk/injection) or Stainless Steel 316?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.

Which is stiffer, Plastic ABS (bulk/injection) or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Stainless Steel 316?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must bePlastic ABS (bulk/injection)Stainless Steel 316
Stiff rod or tie (tension)11.3x heavierlighter
Stiff beam (bending)21% heavierlighter
Stiff panel or platelighter1.74x heavier
Strong rod or tielighter31% heavier
Strong beamlighter2.37x heavier
Strong panel or platelighter3.18x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS (bulk/injection) or Stainless Steel 316?

Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 10% for Plastic ABS (bulk/injection).

Thermal

Which conducts heat better, Plastic ABS (bulk/injection) or Stainless Steel 316?

Stainless Steel 316 conducts heat better: 14.6 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).

Related comparisons