Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS (bulk/injection) · Poisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)
6
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic ABS (bulk/injection) stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against 45 MPa for Plastic ABS (bulk/injection) (8.56x).
Which is lighter, Plastic ABS (bulk/injection) or Steel?
Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Plastic ABS (bulk/injection) or Steel?
Steel is stiffer: Young's modulus 200 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Plastic ABS (bulk/injection) or Steel?
For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
Plastic ABS (bulk/injection)
Steel
Stiff rod or tie (tension)
11.5x heavier
lighter
Stiff beam (bending)
24% heavier
lighter
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
13% heavier
lighter
Strong beam
lighter
1.8x heavier
Strong panel or plate
lighter
2.58x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic ABS (bulk/injection) or Steel?
Steel stretches further before it breaks: 24.2% elongation at break against 10% for Plastic ABS (bulk/injection).
Thermal
Which conducts heat better, Plastic ABS (bulk/injection) or Steel?
Steel conducts heat better: 48 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).