Materials / Compare

Plastic ABS (bulk/injection) vs. Zinc Zamak 3

Compare Plastic ABS (bulk/injection) vs. Zinc Zamak 3 strength, stiffness, weight and thermal properties.

Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
Zinc Zamak 3Cast
MechanicalPlastic ABS (bulk/injection)Zinc Zamak 3
Yield strength45MPa1221MPa24.91x stronger
Ultimate tensile strengthnot stated (yield given)283MPa2
Flexural strength65MPa1not sourced
Elongation at break10%110%2
Young's modulus (stiffness)2.3GPa185.5GPa237.2x stiffer
Density1,040kg/m³16.35x lighter6,600kg/m³2
Strength to weight43.3kN·m/kg29% higher33.5kN·m/kg
Stiffness to weight2.21MN·m/kg13MN·m/kg5.86x higher
Poisson's ratio0.3930.274
Shear modulus0.827GPa33.7GPa40.7x stiffer in shear
Bulk modulus3.48GPa62GPa17.8x higher
Speed of sound1,487m/s3,599m/s2.42x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Zinc Zamak 3
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Zinc Zamak 3
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic ABS (bulk/injection)Zinc Zamak 3
Thermal conductivity0.17W/m·K1113W/m·K2665x more heat through a fin
Thermal expansionrange80–110µm/m·K127.4µm/m·K2
100 mm part over a 50 °C swing475µm growth137µm growth3.47x less
Specific heatnot sourced419J/kg·K2
Heats up and cools (diffusivity)not sourced40.9mm²/s
Thermal shock resistance21.4W/m7,782W/m364x more resistant
Melting pointnot sourcedmelting range381–387°C2
Max service temperatureHDT 1.8 MPa94°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Zinc Zamak 3
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Zinc Zamak 3
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: INEOS Styrolution, Nathan Trotter, Covestro, Eastern Alloys
Plastic ABS (bulk/injection)
INEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)
Zinc Zamak 3
Zamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values
  1. 1
    Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS (bulk/injection) · Yield strength: typical, tensile stress at yield 23 °CPlastic ABS (bulk/injection) · Flexural strength: typical, 23 °CPlastic ABS (bulk/injection) · Elongation at break: nominal strain at break, 23 °CPlastic ABS (bulk/injection) · Young's modulus (stiffness): typicalPlastic ABS (bulk/injection) · Density: typicalPlastic ABS (bulk/injection) · Thermal conductivity: typicalPlastic ABS (bulk/injection) · Thermal expansion: rangePlastic ABS (bulk/injection) · Max service temperature: HDT 1.8 MPa (annealed 4 h/80 °C)
  2. 2
    Zamak 3 Technical Data SheetNathan Trotterarchived copyZinc Zamak 3 · Yield strength: typicalZinc Zamak 3 · Ultimate tensile strength: typicalZinc Zamak 3 · Elongation at break: typical, in 2 in.Zinc Zamak 3 · Young's modulus (stiffness): typicalZinc Zamak 3 · Density: typicalZinc Zamak 3 · Thermal conductivity: typicalZinc Zamak 3 · Thermal expansion: typicalZinc Zamak 3 · Specific heat: typicalZinc Zamak 3 · Melting point: melting range
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS (bulk/injection) · Poisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)
  4. 4
    Zinc Die Casting Properties Guide (2012)Eastern AlloysZinc Zamak 3 · Poisson's ratio: typical, Zamak 3 hot-chamber die cast

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic ABS (bulk/injection) stronger than Zinc Zamak 3?

Zinc Zamak 3 is stronger: its yield strength is 221 MPa against 45 MPa for Plastic ABS (bulk/injection) (4.91x).

Which is lighter, Plastic ABS (bulk/injection) or Zinc Zamak 3?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which is stiffer, Plastic ABS (bulk/injection) or Zinc Zamak 3?

Zinc Zamak 3 is stiffer: Young's modulus 85.5 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Zinc Zamak 3 deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Zinc Zamak 3?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Zinc Zamak 3 is lighter for a stiff rod or tie (tension).

Part that must bePlastic ABS (bulk/injection)Zinc Zamak 3
Stiff rod or tie (tension)5.86x heavierlighter
Stiff beam (bending)lighter4% heavier
Stiff panel or platelighter1.9x heavier
Strong rod or tielighter29% heavier
Strong beamlighter2.2x heavier
Strong panel or platelighter2.86x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Plastic ABS (bulk/injection) or Zinc Zamak 3?

Zinc Zamak 3 conducts heat better: 113 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Zinc Zamak 3 expands less: 27.4 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).

Related comparisons