Plastic ABS vs. Plastic PLA

Compare Plastic ABS vs. Plastic PLA strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
Plastic PLA3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical52.5MPasourcetypical38% stronger
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)52.5MPasourcetypical, peak stress (= stress at yield)38% stronger
Flexural strength61.1MPasourcetypical96.8MPasourcetypical1.58x stronger in bending
Elongation at break4.6%sourcetypical7.8%sourcetypical1.7x more ductile
Young's modulus (stiffness)1.96GPasourcetypical3.25GPasourcetypical1.66x stiffer
Density1,100kg/m³sourcetypical13% lighter1,240kg/m³sourcetypical
Strength to weight34.6kN·m/kg42.3kN·m/kg22% higher
Stiffness to weight1.78MN·m/kg2.62MN·m/kg47% higher
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.706GPanot sourced
Bulk modulus2.97GPanot sourced
Speed of sound1,336m/s1,619m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourced1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Heats up and cools (diffusivity)not sourced0.0874mm²/s
Thermal shock resistance21.2W/mnot sourced
Melting pointnot sourced152°Csourcetypical
Glass transition101°Csourcetypical59.1°Csourcetypical
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)47% hotter58.8°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS and Plastic PLA are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic PLA?

Plastic PLA is stronger: its yield strength is 52.5 MPa against 38.1 MPa for Plastic ABS (38%).

Which is lighter, Plastic ABS or Plastic PLA?

Plastic ABS is lighter: 1,100 kg/m³ against 1,240 kg/m³ for Plastic PLA.

Which is stiffer, Plastic ABS or Plastic PLA?

Plastic PLA is stiffer: Young's modulus 3.25 GPa against 1.96 GPa for Plastic ABS, so the same part in Plastic PLA deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic PLA?

For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSPlastic PLA
Stiff rod or tie (tension)47% heavierlighter
Stiff beam (bending)14% heavierlighter
Stiff panel or plate5% heavierlighter
Strong rod or tie22% heavierlighter
Strong beam10% heavierlighter
Strong panel or plate4% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or Plastic PLA?

Plastic PLA stretches further before it breaks: 7.8% elongation at break against 4.6% for Plastic ABS.

Which handles higher temperatures, Plastic ABS or Plastic PLA?

Plastic ABS does: 86.6 °C against 58.8 °C for Plastic PLA, both HDT 0.455 MPa (printed specimens).

Which conducts heat better, Plastic ABS or Plastic PLA?

Plastic ABS conducts heat better: 0.17 W/m·K against 0.13 W/m·K for Plastic PLA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSPlastic PLA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSPlastic PLA
Strength against density