Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Linatex Premium Rubber Spec Sheet (WMD0118, 2023)Weir MineralsRubber · Ultimate tensile strength: typicalRubber · Elongation at break: typicalRubber · Density: typical (specific gravity)Rubber · Max service temperature: continuous use operating range
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
4
Compressibility of Natural Rubber at Pressures Below 500 kg/cm², J. Res. NBS 68A (1964)National Institute of Standards and Technologyarchived copyRubber · Poisson's ratio: government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation (0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).)Rubber · Specific heat: government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
5
Thermal Conductivity of Soft Vulcanized Natural Rubber: Selected Values (AD 643325)Defense Technical Information Centerarchived copyRubber · Thermal conductivity: government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Nylon PA66 stronger than Rubber?
Plastic Nylon PA66 is stronger: its yield strength is 85 MPa against tensile strength 23 MPa for Rubber (3.7x).
Which is lighter, Plastic Nylon PA66 or Rubber?
Rubber is lighter: 960 kg/m³ against 1,130 kg/m³ for Plastic Nylon PA66.
Which is lighter for the same job, Plastic Nylon PA66 or Rubber?
For the same stiffness or strength: Plastic Nylon PA66 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic Nylon PA66
Rubber
Strong rod or tie
lighter
3.14x heavier
Strong beam
lighter
2.03x heavier
Strong panel or plate
lighter
1.63x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Nylon PA66 or Rubber?
Rubber stretches further before it breaks: 830% elongation at break against 30% for Plastic Nylon PA66.
Thermal
Which conducts heat better, Plastic Nylon PA66 or Rubber?
Plastic Nylon PA66 conducts heat better: 0.33 W/m·K against 0.151 W/m·K for Rubber.