Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: BASF, Cleveland-Cliffs, Covestro, Steel Construction Institute
Plastic Nylon PA66
BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Nylon PA66 stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 85 MPa for Plastic Nylon PA66 (2.84x).
Which is lighter, Plastic Nylon PA66 or Stainless Steel 304?
Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic Nylon PA66 or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 3 GPa for Plastic Nylon PA66, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic Nylon PA66 or Stainless Steel 304?
For the same stiffness or strength: Plastic Nylon PA66 is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic Nylon PA66
Stainless Steel 304
Stiff rod or tie (tension)
9.05x heavier
lighter
Stiff beam (bending)
13% heavier
lighter
Stiff panel or plate
lighter
1.77x heavier
Strong rod or tie
lighter
2.51x heavier
Strong beam
lighter
3.55x heavier
Strong panel or plate
lighter
4.22x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Nylon PA66 or Stainless Steel 304?
Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 30% for Plastic Nylon PA66.
Thermal
Which handles higher temperatures, Plastic Nylon PA66 or Stainless Steel 304?
Stainless Steel 304 does: 899 °C against 101 °C for Plastic Nylon PA66.
Which conducts heat better, Plastic Nylon PA66 or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.