Materials / Compare

Plastic Nylon vs. Plastic Polypropylene

Compare Plastic Nylon vs. Plastic Polypropylene strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon3D printed (FDM)
Plastic PolypropyleneBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength63.1MPasourcetypical33MPasourcetypical, tensile stress at yield ISO 527
Ultimate tensile strength63.1MPasourcetypical, peak stress (= stress at yield)not sourced
Flexural strength82.9MPasourcetypicalnot sourced
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)2.33GPasourcetypical1.45GPasourcetypical, tensile modulus ISO 527
Density1,140kg/m³sourcetypical900kg/m³sourcetypical, 23 °C ISO 1183-1
Strength to weight55.4kN·m/kg1.51x higher36.7kN·m/kg
Stiffness to weight2.04MN·m/kg27% higher1.61MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Shear modulus0.833GPa1.63x stiffer in shear0.511GPa
Bulk modulus3.89GPa3.02GPa
Speed of sound1,430m/s1,269m/s
Thermal
Thermal conductivity0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Thermal expansion98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 C80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
100 mm part over a 50 °C swing500µm growth450µm growth11% less
Specific heat1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)not sourced
Heats up and cools (diffusivity)0.17mm²/snot sourced
Thermal shock resistance53.6W/m1.87x more resistant28.6W/m
Melting point188°Csourcetypicalnot sourced
Glass transition55.1°Csourcetypicalnot sourced
Max service temperature89.2°CsourceHDT 0.455 MPa (printed specimens)90°CsourceHDT 0.45 MPa (ISO 75B), unannealed
Values forUltimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon stronger than Plastic Polypropylene?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against 33 MPa for Plastic Polypropylene (1.91x).

Which is lighter, Plastic Nylon or Plastic Polypropylene?

Plastic Polypropylene is lighter: 900 kg/m³ against 1,140 kg/m³ for Plastic Nylon.

Which is stiffer, Plastic Nylon or Plastic Polypropylene?

Plastic Nylon is stiffer: Young's modulus 2.33 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Plastic Nylon deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Plastic Polypropylene?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate; Plastic Polypropylene is lighter for a stiff panel or plate.

Part that must bePlastic NylonPlastic Polypropylene
Stiff rod or tie (tension)lighter27% heavier
Stiff beam (bending)about equalabout equal
Stiff panel or plate8% heavierlighter
Strong rod or tielighter1.51x heavier
Strong beamlighter22% heavier
Strong panel or platelighter9% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon or Plastic Polypropylene?

Plastic Nylon conducts heat better: 0.33 W/m·K against 0.195 W/m·K for Plastic Polypropylene.

Which expands less with temperature?

Plastic Polypropylene expands less: 90 µm/m·K against 100 µm/m·K for Plastic Nylon.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic NylonPlastic Polypropylene
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic NylonPlastic Polypropylene
Strength against density